# ASME B31G vs RSTRENG: how is corroded pipe assessed?

> ASME B31G and RSTRENG both predict the pressure at which corroded pipe would fail; B31G uses maximum depth and length, RSTRENG the depth profile. A 2009 review for the US pipeline regulator, PHMSA, found RSTRENG the more accurate against burst tests. US pipeline rules (49 CFR 192.712, 195.452) accept both.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T03:06:14+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: Pipelines
- Canonical: https://beacon.winda.ai/library/b31g-vs-rstreng/

## Why does it matter?

Two methods accepted by US rules can give the same corrosion patch different failure pressures, and that number decides whether pipe is repaired, run at lower pressure or left in service [3][6]. A 2009 review for the Pipeline and Hazardous Materials Safety Administration (PHMSA) compared the methods with recorded burst tests [1]. Using actual material properties, the methods based only on depth and length became more likely to overpredict failure pressure as corrosion got deeper; using specified minimum properties and a safety factor, all of them gave safe operating pressures below every recorded burst pressure [1]. Under 49 CFR 192.933, a predicted failure pressure at or below 1.1 times the maximum allowable operating pressure (MAOP) makes a gas pipeline metal loss anomaly an immediate repair condition [6].

## ASME B31G vs RSTRENG at a glance

Modified B31G sits between the two. It came from the same 1989 research project as RSTRENG but, like the original B31G, needs only depth and length [1][2].

| | ASME B31G (original) | Modified B31G | RSTRENG (effective area) |
|---|---|---|---|
| What it is | ASME manual for evaluating metal loss in pressurized pipelines and piping [7] | Revised depth-and-length criterion from American Gas Association (AGA) project PR-3-805, 1989 [1][2] | Profile-based method and software from the same AGA project [2][4] |
| Corrosion input | Maximum depth and overall axial length [1] | Maximum depth and overall axial length [1] | Depth or remaining-wall readings at even spacing along the pipe axis, a "river bottom" profile [1][2] |
| How the shape is treated | Replaced by an idealized curved area for short flaws and a more conservative assumption for long ones [1] | One shape assumption for all lengths, with revised strength and bulging terms; less conservative overall than the original [1][2] | Failure pressure is calculated for every sub-length of the profile and the lowest value kept [1] |
| Accuracy against burst tests (2009 review) | More likely to overpredict as depth increases, with actual properties [1] | Same trend as B31G [1] | Least scatter of the methods reviewed [1] |
| Typical use | Screening and ranking in-line inspection calls [1] | Ranking calls when only length and maximum depth are reported [1] | Detailed assessment when an accurate profile exists [1] |
| Edition named in US rules | ASME/ANSI B31G-1991, reaffirmed 2004 [4] | Not named separately | PR-3-805, 22 December 1989 [4] |
| Current publisher edition | 2023, on stabilized maintenance [7] | Not applicable | 1989 report [4] |

Sources: PHMSA review (2009) [1]; Kiefner and Vieth (1990) [2]; 49 CFR 192.7 and 195.3 [4]; ASME product page [7].

## When is ASME B31G used?

- **To screen and rank anomalies after an in-line inspection.** The 2009 review concluded that B31G and Modified B31G can continue to serve this purpose [1].
- **When only overall length and maximum depth are known,** as in many inspection summaries [1].
- **To calculate temporary pressure reductions.** For liquid lines in high consequence areas, 49 CFR 195.452(h) requires the reduction to be calculated with the referenced methods, which include B31G and RSTRENG [5].
- **Beyond pipelines.** ASME states that the manual applies to piping systems within the B31 code family, including B31.4, B31.8, B31.11 and the pipeline part of B31.12 [7].

## When is RSTRENG used?

- **When the corroded area has been profiled,** for example by depth readings taken at regular intervals in the ditch [2].
- **To remove excess conservatism.** Its developers described the original B31G as overconservative and built RSTRENG and the modified criterion to bring predictions closer to burst test results [2].
- **For higher-strength pipe.** The 2009 review suggested RSTRENG for grades above X65 because, with specified minimum properties, its predictions stayed below recorded failure pressures for machined defects in pipe up to grade X100 [1].

Its developers found it better at predicting ruptures than leaks, which the 2009 review links to the underlying equation not working well for very deep defects [1].

## What do both methods leave out?

- **Cracks and dents.** 49 CFR 192.712 lists B31G and RSTRENG for corrosion metal loss only; dents and mechanical damage need an engineering critical assessment, and cracks need a fracture mechanics model [3].
- **Uncertainty in the inputs.** The same section requires operators to account for tool tolerance, detection threshold, probability of detection and sizing accuracy unless the flaw was measured directly [3].
- **Missing records.** Pipe properties must come from traceable, verifiable and complete records; otherwise conservative defaults apply, such as assuming Grade A pipe (30,000 psi) [3].
- **Closely spaced flaws.** The original B31G had no rule for interaction between nearby anomalies [2].
- **Modern steels.** The test database behind B31G, Modified B31G and RSTRENG was dominated by older, lower-strength, lower-toughness steels [1].

Gas transmission rules also send the result back to the pipe: where corrosion leaves less wall than the MAOP needs, the pipe must be repaired, replaced or run at lower pressure, with strength determined under 192.712 [9].

## Where integrity problems show up

| Decision | Data it depends on | What goes wrong without it |
|---|---|--- |
| Which flaw depth goes into the calculation | Inspection sizing plus the tool's stated tolerance, or a field measurement | Marshall, Michigan, 2010: crack depths from a 2005 inspection were used as reported, without the tool tolerance; NTSB noted this can put predicted failure pressure above the actual one, so defects are not dug [8] |
| Which wall thickness and strength to use | Traceable, verifiable and complete pipe records | Same case: using a tool-reported wall of 0.285 inch instead of the 0.25 inch nominal wall added about 14% to the segment's pressure rating [8] |
| Which method fits the flaw | Anomaly type from inspection and digs | Corrosion methods do not cover dents or cracks; 192.712 requires separate analyses for them [3] |
| Repair, reduce pressure or monitor | Predicted failure pressure compared with MAOP or maximum operating pressure | Gas: at or below 1.1 times MAOP is an immediate repair condition [6]. Liquid: a predicted burst pressure below maximum operating pressure is immediate [5] |
| Whether nearby pits act as one flaw | Spacing of corrosion features | Treating separate pits as one area is overly conservative; treating them apart may be nonconservative [2] |

Sources: NTSB PAR-12/01 (2012) [8]; 49 CFR 192.712, 192.933, 195.452 [3][5][6]; Kiefner and Vieth (1990) [2].

## Sources

1. [A Review of Methods for Assessing the Remaining Strength of Corroded Pipelines, Report 6781, Issue 6.1 (V. Chauhan, J. Brister), prepared for PHMSA under DTPH56-05-T0003, Project 153, GL Industrial Services for the US Pipeline and Hazardous Materials Safety Administration (PHMSA)](https://primis.phmsa.dot.gov/rd/FileGet/5278/Report_6781_Issue_6_1_Final.pdf)
2. [Evaluating pipe, conclusion: PC program speeds new criterion for evaluating corroded pipe (J. F. Kiefner, P. H. Vieth), Oil & Gas Journal](https://www.ogj.com/home/article/17214053/evaluating-pipe-conclusion-pc-program-speeds-new-criterion-for-evaluating-corroded-pipe), 1990-08-20
3. [49 CFR 192.712, Analysis of predicted failure pressure and critical strain level, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/section-192.712)
4. [49 CFR 192.7 and 195.3, What documents are incorporated by reference, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/section-192.7)
5. [49 CFR 195.452, Pipeline integrity management in high consequence areas, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/section-195.452)
6. [49 CFR 192.933, What actions must be taken to address integrity issues?, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/section-192.933)
7. [B31G, Manual for Determining the Remaining Strength of Corroded Pipelines (product page) (2023 edition listed (editions 2009, 2012 and 2023 shown); placed on stabilized maintenance), American Society of Mechanical Engineers (ASME)](https://www.asme.org/codes-standards/find-codes-standards/b31g-manual-determining-remaining-strength-corroded-pipelines)
8. [Pipeline Accident Report NTSB/PAR-12/01: Enbridge Incorporated Hazardous Liquid Pipeline Rupture and Release, Marshall, Michigan, July 25, 2010, US National Transportation Safety Board (NTSB)](https://www.ntsb.gov/investigations/AccidentReports/Reports/PAR1201.pdf), 2012-07-10
9. [49 CFR 192.485, Remedial measures: Transmission lines, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/section-192.485)

Published by Winda Beacon (https://beacon.winda.ai).