> Corrosion control keeps metal loss and cracking slow enough for equipment to reach its design life. The main methods are resistant materials and design, protective coatings, cathodic protection, corrosion inhibitors, changing the environment, and monitoring to confirm they work. In the US, 49 CFR 192 Subpart I and 195 Subpart H set minimum pipeline requirements.

- Label: Fact
- Type: Explainer
- Published: 2026-11-14T11:53:52+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-14
- Topics: Pipelines, Upstream and offshore
- Canonical: https://beacon.winda.ai/library/corrosion-control-methods/

## Why does it matter?

From 1998 to 2017, corrosion caused about 18% of US pipeline incidents on average, according to the Pipeline and Hazardous Materials Safety Administration (PHMSA) [2]. PHMSA attributes about 60% of corrosion-caused incidents on transmission and gathering lines to internal corrosion [3], which a coating or cathodic protection on the outside of the pipe does not reach. The same agency states that steel pipelines can last indefinitely when protective measures stay effective [2].

## How does corrosion control work?

Corrosion of steel in soil or water behaves like a battery. Metal dissolves at an anode, a reaction such as oxygen reduction consumes the electrons at a cathode, the steel connects the two, and the soil or water (the electrolyte) completes the circuit [5]. Each control method removes or weakens one part of this cell [9]. A coating separates steel from electrolyte, cathodic protection makes the whole surface a cathode, an inhibitor acts at the wetted surface, and dehydration, scavengers or biocides remove what the reactions need [3][4][5][9][13].

Materials and design act first: a metal suited to the environment, and shapes that do not trap water [1][6]. The UK National Physical Laboratory (NPL) notes that corrosion cannot always be prevented, but it can always be controlled sufficiently [1].

## What are the main methods of corrosion control?

| Method | What it acts on | Typical use in oil and gas | Main limit | In the Library |
|---|---|---|---|---|
| Materials and design | The metal itself; shape, drainage and extra wall thickness (corrosion allowance) | Corrosion-resistant alloys in aggressive wells; allowance on carbon steel structures and equipment [6][9] | An alloy normally doubles material cost or more [6]; an allowance covers general, not localized, loss [1] | [How are materials selected for oil and gas equipment?](/library/material-selection/), [Corrosion allowance](/glossary/corrosion-allowance/) |
| Protective coatings | Contact between the steel and its environment | Pipeline coatings and tapes, paint systems on structures and plant [5][1] | Holidays, damage, disbonding; a coating usually wears out well before the plant it protects reaches the end of its life [1][10] | [How do protective coatings prevent corrosion?](/library/protective-coatings/) |
| Cathodic protection | The electrical potential of the steel, set by sacrificial anodes or impressed current | Buried and submerged pipelines, tank bases, jetties, offshore structures [4] | Needs a surrounding electrolyte, so it cannot stop atmospheric corrosion; shielded steel gets no current [4][10] | [How does cathodic protection work?](/library/cathodic-protection/), [Sacrificial anode vs impressed current cathodic protection](/library/sacrificial-vs-impressed-current/) |
| Corrosion inhibitors | Reactions at the wetted metal surface | Wells and pipelines carrying water with carbon dioxide (CO2) or hydrogen sulfide (H2S) [9][12] | Not effective against oxygen corrosion or microbiologically influenced corrosion (MIC); high flow, heat and solids reduce the effect [12] | [How do corrosion inhibitors work?](/library/corrosion-inhibitors/) |
| Changing the environment | Water, oxygen, contaminants and microbes in the fluid | Product quality control, cleaning pigs, oxygen scavengers, biocides [3][9][13] | Liquids and solids still collect where pigs cannot run [11] | [How are biocides used to control microbiologically influenced corrosion?](/library/biocides-for-mic/) |
| Monitoring and inspection | Whether the other methods work | Coupons and probes, pipe-to-soil potential surveys, in-line inspection [3][7] | Readings are local: a test station 100 feet from the 2012 Sissonville rupture read satisfactory for 10 years [10] | [What is corrosion monitoring and which methods are used?](/library/corrosion-monitoring/) |

Sources: NPL Guides No. 1, 4 and 11 [1][4][5]; PHMSA [3]; NASA [6]; eCFR [7]; Solovyeva et al., 2023 [9]; NTSB [10][11]; HSE RR1023 [12]; Shi et al., 2023 [13].

## How are the methods combined?

- **Coating plus cathodic protection.** A good coating cuts the current cathodic protection needs and lets it spread further; NPL calls the pair normally the most practical and economic system [4]. US rules require both on buried gas pipelines installed after July 31, 1971 (49 CFR 192.455) [7].
- **Inhibitors plus monitoring.** Hazardous liquid operators using inhibitors must dose the whole system they serve and examine coupons at least twice a year (49 CFR 195.579) [8].
- **Alloys plus inhibitors.** Corrosion-resistant alloys in severe wells are still dosed with inhibitors during acid treatments, which can affect them [9].
- **Cleaning plus product control.** Operators run cleaning pigs, control product moisture and chemistry, and sometimes inject inhibitors [3].

## How is a method chosen?

NASA's Kennedy Space Center corrosion laboratory notes that the choice depends on economics, safety requirements and technical factors [6].

- **The environment limits the options.** Cathodic protection needs soil, water or concrete around the steel; exposed pipe must instead be cleaned and coated [4][7].
- **Early decisions cost less.** NPL puts effective external corrosion control at about 1 to 2% of the cost of laying a pipeline [5]. New onshore US gas transmission lines built since May 2007 must limit where liquids collect and allow internal corrosion monitoring (49 CFR 192.476) [7].
- **Surveys come first.** For buried pipelines, NPL describes surveying soil resistivity, chemistry, bacteria and stray currents before the protective system is fixed [5].

## What do US pipeline rules require?

Gas lines need cathodic protection meeting Appendix D to Part 192, tested every calendar year, with rectifiers checked six times a year (49 CFR 192.463, 192.465) [7]. Corrosive gas may be carried only after its effect is investigated, with coupons checked twice a year (49 CFR 192.475, 192.477) [7]. Exposed pipe is generally cleaned and coated, and onshore pipe is inspected at least every 3 calendar years (49 CFR 192.479, 192.481); Part 195 has parallel rules for hazardous liquids [7][8].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Buried, coated gas line in rocky backfill [10] | Rocks damaged the coating and shielded the steel from impressed current; over 70% wall loss [10] | In-line inspection or a pressure test, which the NTSB concluded would likely have revealed it [10] | [How does cathodic protection work?](/library/cathodic-protection/) |
| Low points in a gas transmission line [11] | Water, chlorides, oxygen, CO2, H2S and microbes collected where cleaning pigs could not run; no inhibitor or coupons were used [11] | Coupons or probes, in-line inspection, wall thickness measurement, inspection when pipe is opened [11] | [What is microbiologically influenced corrosion (MIC)?](/library/microbiologically-influenced-corrosion/) |
| Pipe at soil-to-air interfaces, supports, splash zones, under insulation or disbonded coating | Coating breakdown where cathodic protection cannot act [4][5] | Visual inspection at least every 3 calendar years onshore, every year offshore (49 CFR 192.481) [7] | [What is atmospheric corrosion?](/library/atmospheric-corrosion/) |
| Coated pipe backfilled after a repair or replacement of 1,000 feet or more | Coating damage during handling and backfill [7] | Direct or alternating current voltage gradient survey within 6 months (49 CFR 192.461(f)) [7] | [Coating holiday](/glossary/coating-holiday/) |
| Pipelines near electric railways, other cathodic protection systems or power lines | Stray current leaving the pipe into the soil speeds corrosion there [5] | Interference surveys (49 CFR 192.473(c)) [7] | [What is soil corrosion?](/library/soil-corrosion/) |

Sources: NTSB PAR-14/01 [10] and PAR-03/01 [11]; NPL Guides No. 1 and 4 [4][5]; 49 CFR 192 Subpart I [7].

## Sources

1. [Guides to Good Practice in Corrosion Control No. 11: Corrosion control checklist, National Physical Laboratory (NPL), UK](https://eprintspublications.npl.co.uk/8621/1/Corrosion%20Guide%20No%2011.pdf)
2. [Fact Sheet: Corrosion, US Pipeline and Hazardous Materials Safety Administration (PHMSA)](https://primis.phmsa.dot.gov/stakeholder-comms/factsheets/fscorrosion)
3. [Fact Sheet: Internal Corrosion, US Pipeline and Hazardous Materials Safety Administration (PHMSA)](https://primis.phmsa.dot.gov/stakeholder-comms/factsheets/fsinternalcorrosion)
4. [Guides to Good Practice in Corrosion Control No. 1: Cathodic Protection (D. W. Harvey), National Physical Laboratory (NPL), UK](https://eprintspublications.npl.co.uk/8402/1/Corrosion%20Guide%20No%201.pdf)
5. [Guides to Good Practice in Corrosion Control No. 4: Corrosion Control for Buried Pipelines (D. W. Harvey), National Physical Laboratory (NPL), UK](https://eprintspublications.npl.co.uk/8622/1/Corrosion%20Guide%20No%204.pdf)
6. [Corrosion Control, NASA Kennedy Space Center, Corrosion Technology Laboratory](https://public.ksc.nasa.gov/corrosion/corrosion-control/)
7. [49 CFR Part 192, Subpart I, Requirements for Corrosion Control (192.451 to 192.493), eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/chapter-I/subchapter-D/part-192/subpart-I)
8. [49 CFR Part 195, Subpart H, Corrosion Control (195.551 to 195.591), eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/chapter-I/subchapter-D/part-195/subpart-H)
9. [Current Downhole Corrosion Control Solutions and Trends in the Oil and Gas Industry: A Review (V. A. Solovyeva, K. H. Almuhammadi, W. O. Badeghaish), Materials 16(5):1795, MDPI (open access, CC BY 4.0)](https://pmc.ncbi.nlm.nih.gov/articles/PMC10004626/), 2023-02-22
10. [Pipeline Accident Report NTSB/PAR-14/01: Columbia Gas Transmission Corporation Pipeline Rupture, Sissonville, West Virginia, December 11, 2012, US National Transportation Safety Board (NTSB)](https://www.ntsb.gov/investigations/AccidentReports/Reports/PAR1401.pdf)
11. [Pipeline Accident Report NTSB/PAR-03/01: Natural Gas Pipeline Rupture and Fire Near Carlsbad, New Mexico, August 19, 2000, US National Transportation Safety Board (NTSB)](https://www.ntsb.gov/investigations/AccidentReports/Reports/PAR0301.pdf)
12. [RR1023: Reliable corrosion inhibition in the oil and gas industry (J. Hobbs, Health and Safety Laboratory, 2014; archived copy, withdrawn from hse.gov.uk), UK Health and Safety Executive (HSE)](http://web.archive.org/web/20240809100026id_/https://www.hse.gov.uk/research/rrpdf/rr1023.pdf)
13. [Comprehensive Review on the Use of Biocides in Microbiologically Influenced Corrosion (X. Shi, R. Zhang, W. Sand and others), Microorganisms 11(9):2194, MDPI (open access, CC BY 4.0)](https://pmc.ncbi.nlm.nih.gov/articles/PMC10535546/), 2023-08-30