# Corrosion coupons vs electrical resistance (ER) probes

> A corrosion coupon is a metal sample weighed before and after exposure for an average rate; an electrical resistance (ER) probe tracks metal loss in place. Coupons need retrieval and laboratory work; ER probes read their element's thinning without removal. Both measure a sample at one point, and US pipeline rules (49 CFR 192.477) accept coupons or equivalent means.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T09:26:54+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: LNG, Pipelines, Refining, Upstream and offshore
- Canonical: https://beacon.winda.ai/library/corrosion-coupons-vs-er-probes/

## Why does it matter?

A clean coupon result does not prove there was no corrosive episode. A coupon reports one average rate for its whole exposure, which a 2019 review by researchers at the US National Energy Technology Laboratory (NETL) puts at a few months, with no real-time information [1]. ASTM's public scope text for its online monitoring guide describes ER readings as a way to spot corrosive process upsets early, without entering the system to pull samples [2]. US pipeline rules require coupons or other suitable means wherever gas is corrosive, and wherever liquid lines rely on inhibitors [4][5].

## Corrosion coupons vs ER probes at a glance

| | Corrosion coupon | Electrical resistance (ER) probe |
|---|---|---|
| What it is | A small metal piece with a prepared surface, placed in the stream during operation [6] | A metal element wired so its electrical resistance can be read; the NETL review calls it an "electrical" coupon [1] |
| What it measures | Mass lost during the exposure, after corrosion products are cleaned off [1][3] | The rise in resistance as the element thins, giving cumulative metal loss [1][2] |
| Main result | One average corrosion rate for the exposure period [1] | A metal loss trend; the rate is inferred from it [2] |
| Time to a result | After retrieval and laboratory analysis; a few months per exposure in the NETL review [1] | Continuous or periodic readings without removal [2] |
| Form of attack | The cleaned coupon can be examined for pitting as well as mass loss [3] | Common elements measure uniform corrosion; designs sensitive to local attack are still in research [1] |
| Where it works | Made in the material and shape of interest [1] | Conductive and non-conductive media, such as produced water, oil, gas and air [1] |
| Data | Weighing and records by hand [1] | Electronic logging, local or remote [1][2] |
| Main limits | Slow; one location; no information inside the exposure [1] | One location; electronics need upkeep; intrinsic safety rules apply in flammable areas [1] |
| US pipeline rules | Named in 49 CFR 192.477 and 195.579 [4][5] | Not named; the same rules also allow "other suitable means" (192.477) or "other monitoring equipment" (195.579) [4][5] |

Sources: Wright et al., 2019 [1]; ASTM G96 and G1 product pages [2][3]; 49 CFR 192.477 and 195.579 [4][5]; NTSB/PAR-03/01 [6].

## When are corrosion coupons used?

- **As the reference measurement.** The NETL review describes coupon weight loss as the most established and longest-used method, still treated as the standard against which other monitoring methods are judged [1].
- **To see the type of attack.** After cleaning, a coupon can be weighed and examined for pits, which ASTM's specimen practice covers [3].
- **To meet US pipeline monitoring rules.** Coupons, or other means, check internal corrosion control on corrosive gas lines and inhibitor programs on liquid lines, at least twice each calendar year with no more than 7.5 months between checks [4][5].

## When are ER probes used?

- **When readings are needed without entering the system.** ER readings come without withdrawing anything, unlike coupons [2].
- **To catch process upsets and steer inhibitor dosing.** ASTM's scope text cites early warning of corrosive conditions and signaling when more inhibitor is needed [2].
- **In streams that do not conduct electricity.** ER elements work in gas, oil and air, where electrochemical probes such as linear polarization resistance (LPR) need a conductive liquid [1].
- **Where data should be logged or sent remotely** [1][2].

## What do both methods have in common?

Both are point sensors: they report what happens to a sample at the spot where it is installed, and the NETL review notes that positions are usually chosen from experience, so unusual corroding spots can be missed [1]. ASTM's guide adds that a rate from a coupon or a probe element is an average over its surface, so the sample has to be looked at to judge how uneven the attack was [2]. Neither measures the wall of the pipe or vessel itself; that is the job of inspection methods such as [ultrasonic thickness measurement](/library/ultrasonic-thickness-measurement/).

## Where integrity problems show up

| What it finds well | What it can miss or get wrong | In the Library |
|---|---|---|
| Coupon: average corrosion rate at its location, and pits seen once it is cleaned [1][3] | Short corrosive episodes inside a months-long exposure [1] | [What is corrosion monitoring and which methods are used?](/library/corrosion-monitoring/) |
| ER probe: metal loss trend without removal, early warning of upsets [2] | Pitting and other local attack on common elements [1] | [What is pitting corrosion?](/library/pitting-corrosion/) |
| Both: how corrosive the stream is at the sample point [1] | Corrosion where liquids collect away from the sample; at Carlsbad, New Mexico, in 2000, liquids gathered at a low point formed by a pipe bend, a section with no coupons [6] | [What is microbiologically influenced corrosion (MIC)?](/library/microbiologically-influenced-corrosion/) |
| Both: whether an inhibitor program is working [2][5] | The actual wall of the equipment, which neither measures [1] | [How does ultrasonic thickness measurement work?](/library/ultrasonic-thickness-measurement/) |

Sources: Wright et al., 2019 [1]; ASTM G96 and G1 product pages [2][3]; 49 CFR 195.579 [5]; NTSB/PAR-03/01, 2003 [6].

## Sources

1. [Corrosion Sensors for Structural Health Monitoring of Oil and Natural Gas Infrastructure: A Review (R. F. Wright et al.), Sensors 19(18):3964, MDPI, via PubMed Central](https://pmc.ncbi.nlm.nih.gov/articles/PMC6767297/), 2019-09-13
2. [ASTM G96-90(2018), Standard Guide for Online Monitoring of Corrosion in Plant Equipment (Electrical and Electrochemical Methods) (product page, Scope and Significance) (G96-90 (reapproved 2018), marked historical on the ASTM store), ASTM International](https://store.astm.org/g0096-90r18.html)
3. [ASTM G1-03(2017)e1, Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens (product page, Scope and Significance) (G1-03 (reapproved 2017), editorially corrected; marked historical on the ASTM store), ASTM International](https://store.astm.org/g0001-03r17e01.html)
4. [49 CFR 192.477, Internal corrosion control: Monitoring, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/section-192.477)
5. [49 CFR 195.579, What must I do to mitigate internal corrosion?, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/section-195.579)
6. [Pipeline Accident Report: Natural Gas Pipeline Rupture and Fire Near Carlsbad, New Mexico, August 19, 2000 (NTSB/PAR-03/01), US National Transportation Safety Board (NTSB)](https://www.ntsb.gov/investigations/AccidentReports/Reports/PAR0301.pdf)

Published by Winda Beacon (https://beacon.winda.ai).