# What is crevice corrosion?

> Crevice corrosion is localized corrosion inside a narrow gap, such as under a gasket, washer, clamp or deposit, where trapped liquid stagnates. Oxygen inside the gap is used up, chloride gathers and the liquid turns acidic, so the metal in the gap corrodes while nearby surfaces stay protected. Stainless steels are especially prone.

- Label: Fact
- Type: Explainer
- Published: 2026-11-14T11:57:56+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-14
- Topics: LNG, Refining, Upstream and offshore
- Canonical: https://beacon.winda.ai/library/crevice-corrosion/

## Why does it matter?

Stainless steels resist corrosion because of a thin passive film, and a tight gap can defeat it. The UK National Physical Laboratory (NPL) notes that type 316 stainless steel is usable in seawater, yet crevices in it can corrode unless the steel is cathodically protected [2]. NASA's corrosion laboratory adds that stainless steels are always susceptible to this attack, because, unlike pitting, it needs no pit nucleus to start [1]. Once it starts, NPL says it behaves like pitting and can grow very fast [2], and it does so inside joints that routine external checks do not see [3].

## How does crevice corrosion start and grow?

A crevice forms where two parts sit close together and water collects in the gap between them; if the gap is narrow enough, the water inside ends up with less oxygen than the water outside [8][2]. From there the attack builds in three stages:

1. **Oxygen runs out.** The liquid trapped in the joint quickly loses its dissolved oxygen, and metal inside starts to dissolve faster. The gap becomes the anode and the open surface around it the cathode, a differential aeration cell [2][8][4].
2. **Chemistry turns hostile.** NASA describes the liquid inside pits, crevices and cracks becoming richer in chloride and more acidic than the surroundings [1]. NPL reports that where type 316 is joined tightly to a super-austenitic grade and the joint sits in seawater, crevice corrosion can push the pH below 1 [5].
3. **The attack speeds up.** Once started, crevice corrosion behaves much like pitting, where an acidic, chloride-rich liquid dissolves metal fast, and NPL notes that very high growth rates are possible [2].

NPL describes a second form found on copper alloys: a metal-ion concentration cell, where the corrosion appears just outside the gap instead of inside it [2].

## Which materials are most at risk?

| Material | Crevice behavior in seawater | Source |
|---|---|---|
| Type 304 stainless steel | Unsuitable for seawater service | NPL [2] |
| Type 316 and 316L stainless steel | Better than 304 because of molybdenum; usable in seawater but can crevice-corrode unless cathodically protected | NASA [1], NPL [2] |
| Alloy 400, alloy K-500, alloy 825 and 22Cr duplex stainless steel | Grouped with 316 by NPL as corrosion resistant but susceptible to crevice corrosion in seawater | NPL [2][5] |
| Super-austenitic and super duplex stainless steels, nickel-chromium-molybdenum alloys with more than 7% molybdenum, titanium | Grouped by NPL as noble and passive in seawater, apart from the crevice-susceptible group; the stainless grades in this group have a pitting resistance equivalent number (PREN, calculated from chromium, molybdenum, tungsten and nitrogen) above 40, and alloy 625 has excellent seawater crevice resistance | NPL [2][5] |
| Titanium alloys in general | A common aerospace grade crevice-corroded where a more resistant grade was needed; special alloying additions give crevice resistance at high temperature | NASA [1] |
| Copper alloys | Attack tends to occur just outside the gap | NPL [2] |

In NPL's guidance on mixed-metal joints in seawater, alloys of the crevice-susceptible group are protected from crevice corrosion when coupled to a less noble metal with a large enough anode area [5].

## How is crevice corrosion found?

The hard part is that the attack sits on faces nobody can see without taking something apart. NASA's corrosion laboratory lists where it forms: under washers, under applied films, beneath sand grains or barnacles, and in the pockets of threaded joints [1]. The US National Institute of Standards and Technology (NIST) gives the crevice under a weld backing strip as an example of localized attack in a place that is hard to inspect [3].

Outward signs come late. The US Federal Aviation Administration's corrosion guide, written for aircraft but describing the same mechanism, notes that corrosion inside a joint usually shows first as bulging of the thin metal over it, or as corrosion products seeping out of the gap through which the water got in [7]. Where it is practicable, the guide asks for the joined surfaces to be separated so the attack can be treated and stopped [7].

Design decides how much of this is possible. NPL's corrosion checklist links the shapes that trap liquid with poor access for inspection and repair, and asks designers to leave access to every part of a structure, so that material can be replaced where the risk and the consequences of corrosion are significant [4].

## How is crevice corrosion prevented?

- **Design out the gap.** NPL's checklist warns that stitch welds, poor weld profiles and lack of fusion create crevices, and that joints dry slowly and concentrate salts [4].
- **Seal it.** Sealants and jointing compounds keep water out of lap joints and fastener seats [1][5].
- **Choose the alloy for the water.** Molybdenum-bearing and higher-alloy grades resist crevice attack better [1][2].
- **Keep surfaces clean and coated** [1].
- **Protect it cathodically** where 316 is used in seawater [2].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Pressure vessel welds made with backing strips | The gap left under the backing material [3] | Hard to inspect; NIST cites it as an example of hidden local attack [3] | [How are pressure vessels inspected?](/library/pressure-vessel-inspection/) |
| Offshore risers | Wetting and drying in the splash zone and coating defects; crevice corrosion is on the list of expected riser mechanisms [6] | Methods reviewed for risers in a 2003 study for US offshore regulators [6] | [What are the main non-destructive testing (NDT) methods in oil and gas?](/library/ndt-methods-overview/) |

Sources: NIST SP 780, 1990 [3]; NPL Guide 6, 2020 [2]; MMS TAP 433, 2003 [6].

## Sources

1. [Forms of Corrosion, NASA Kennedy Space Center, Corrosion Technology Laboratory](https://public.ksc.nasa.gov/corrosion/forms-of-corrosion/)
2. [Guides to Good Practice in Corrosion Control No. 6: Corrosion Control for Pumps and Valves, UK National Physical Laboratory (NPL)](https://eprintspublications.npl.co.uk/8618/1/Corrosion%20Guide%20No%206.pdf)
3. [NIST Special Publication 780, Guidelines for Pressure Vessel Safety Assessment (S. Yukawa), US National Institute of Standards and Technology (NIST)](https://nvlpubs.nist.gov/nistpubs/Legacy/SP/nistspecialpublication780.pdf)
4. [Guides to Good Practice in Corrosion Control No. 11: Corrosion control checklist, UK National Physical Laboratory (NPL)](https://eprintspublications.npl.co.uk/8621/1/Corrosion%20Guide%20No%2011.pdf)
5. [Guides to Good Practice in Corrosion Control No. 5: Bimetallic Corrosion, UK National Physical Laboratory (NPL)](https://eprintspublications.npl.co.uk/8617/1/Corrosion%20Guide%20No.5.pdf)
6. [Evaluation of Methods for Detecting and Monitoring of Corrosion and Fatigue Damage in Risers (M. Lozev and others), Technology Assessment Program (TAP) Project 433, US Minerals Management Service (now BSEE)](https://www.bsee.gov/sites/bsee.gov/files/tap-technical-assessment-program//433aa.pdf), 2003-11-04
7. [Advisory Circular AC 43-4B, Corrosion Control for Aircraft, US Federal Aviation Administration (FAA)](https://www.faa.gov/documentLibrary/media/Advisory_Circular/AC_43-4B.pdf), 2018-09-11
8. [Crevice corrosion, School of Materials Science and Engineering, UNSW Sydney](https://www.materials.unsw.edu.au/crevice-corrosion)

Published by Winda Beacon (https://beacon.winda.ai).