# HIC vs SOHIC vs SSC: how do hydrogen sulfide cracking forms differ?

> HIC, SOHIC and SSC are cracking caused by hydrogen entering steel from wet hydrogen sulfide (H2S) corrosion. Hydrogen-induced cracking (HIC) needs no stress and runs parallel to the surface; stress-oriented HIC (SOHIC) stacks such cracks through the wall under stress; sulfide stress cracking (SSC) splits hard, stressed steel. NACE MR0175/ISO 15156 covers production materials.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T15:18:43+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: LNG, Pipelines, Refining, Upstream and offshore
- Canonical: https://beacon.winda.ai/library/hic-vs-sohic-vs-ssc/

## Why does it matter?

Steel ordered as resistant to hydrogen-induced cracking is not automatically resistant to its stress-oriented form: a 2022 review published by the US National Institute of Standards and Technology (NIST) notes that such steel can still crack near welds and at high stress [1]. The forms also combine: in the amine absorber that ruptured at Romeoville, Illinois, in 1984, killing 17 people, investigators traced cracks that began in hard metal beside a repair weld and then grew through the wall by hydrogen pressure cracking [4][9].

## HIC vs SOHIC vs SSC at a glance

All three start the same way: corrosion in water containing H2S produces hydrogen atoms, and H2S keeps them from pairing up at the surface, so many enter the steel [1][2].

| | HIC | SOHIC | SSC |
|---|---|---|---|
| What happens | Hydrogen gathers at inclusions, forms gas, and gas pressure opens cracks [1] | Small HIC-type cracks form in stacks and link through the wall [1] | Absorbed hydrogen embrittles hard steel under tension and a crack runs across it [6][7] |
| Stress needed | No applied stress [1] | Yes, applied or residual; reported at hoop stress as low as 30% of yield [1] | Yes, tensile stress [6] |
| Main material factor | Sulfur and inclusions, center-line segregation, banded microstructure [1] | Uneven microstructure and local strain; HIC resistance alone is not enough [1] | Hardness and strength [2][3] |
| How it is usually found | Ultrasonic testing for internal in-plane cracks; blisters seen on the surface [2][5] | Wet fluorescent magnetic particle testing of weld surfaces, plus ultrasonic methods to size depth [2][8] | Wet fluorescent magnetic particle testing of welds; hardness testing, which can miss very small hard zones [2][3] |

Sources: Martin and Sofronis (NIST), 2022 [1]; NIST SP 780 [2]; OSHA Technical Manual [3]; Kazys and others, 2022 [5]; 30 CFR 250.490 [6]; Kaley and others, 1996 [8].

## When does HIC occur?

- **In low- to medium-strength steel with no applied load.** The driving force is hydrogen gas pressure inside the crack [1].
- **Where the steel gives hydrogen somewhere to collect.** Elongated manganese sulfide inclusions are the most common start points; center-line segregation and banded structures add risk, and banding in steel harder than 300 on the Vickers scale (HV) can matter more than sulfur content [1].
- **When uptake is high.** Uptake depends on temperature, pH, solution chemistry and the partial pressures of H2S, carbon dioxide and hydrogen, not necessarily the total pressure [1].
- **Near the surface, as blisters.** Small blisters seldom threaten strength because the voids lie parallel to the wall, but they show that hydrogen is entering [2]. Failure becomes possible when stepwise cracking cuts the effective wall thickness [1].

## When does SOHIC occur?

- **At modest stress.** The NIST review cites SOHIC at hoop stress as low as 30% of yield, and notes that stress can cause cracking in conditions too mild to cause HIC alone [1].

## When does SSC occur?

- **In hard or high-strength steel under tension.** NIST lists high-strength bolts and the heat-affected zones of welds without PWHT as susceptible conditions [2].
- **At small hard spots in welds.** The US Occupational Safety and Health Administration (OSHA) notes that significant cracks can start at very small hard zones that conventional hardness tests do not detect [3].
- **In sour production equipment.** US offshore rules require equipment in H2S zones to resist SSC, cite NACE MR0175 for blowout preventer, wellhead and pressure-control equipment, and require welding done in a way that keeps SSC resistance (30 CFR 250.490(p)) [6].
- **Where the environment drives more hydrogen in.** pH, temperature and H2S partial pressure all affect hydrogen entry [7].

## How is each form found?

Different forms need different methods, and no single one sees everything. In a Materials Properties Council research program on welded plate exposed to H2S, combined ultrasonic methods measured the size, depth and position of HIC, SOHIC and SSC well; automated scans were more repeatable than manual ones; and no single ultrasonic method described the damage fully [8]. On refinery heat exchanger steel in 2022, total focusing method imaging resolved cracks close to 0.2 mm, a low-angle time-of-flight diffraction probe suited screening of large areas, and the velocity ratio method missed a thin damaged layer [5].

When investigators examined the 1984 absorber, magnetic particle testing showed several hundred cracks near the field repair welds and few near the original welds, ultrasonic testing found widespread internal separation in one shell course, and wall thickness showed no significant loss [4].

## Is SOHIC a kind of HIC or a kind of SSC?

The NIST review notes that SOHIC has been described as a mix of HIC and SSC, but that acoustic emission evidence points to a mechanism close to HIC [1]. Both agree on its shape: in-plane HIC cracks that stress lines up into a through-wall column [1]. Older names such as stepwise cracking, blister cracking and hydrogen pressure cracking all fall under HIC in NACE terminology [1].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Refinery amine absorbers and vessels repaired by welding | Hard, untempered repair-weld zones; hydrogen-charged plate with earlier blisters [4] | Magnetic particle testing showed several hundred cracks near repair welds; ultrasonic testing showed internal separation [4] | [What is an amine gas treating unit?](/library/amine-gas-treating/) |
| Liquefied petroleum gas (LPG) storage spheres | H2S believed carried over from treating; weld heat-affected zones; higher-strength steels [2][3] | Wet fluorescent magnetic particle testing; early inspection recommended for spheres in service over 5 years [2][3] | [Sulfide stress cracking](/glossary/sulfide-stress-cracking/) |
| Welds and welded attachments in vessel plate | Residual stress and heat-affected zones in wet H2S [8] | Manual and automated ultrasonic testing with magnetic particle testing, confirmed by sectioning in research tests [8] | [Stress oriented hydrogen induced cracking](/glossary/stress-oriented-hydrogen-induced-cracking/) |
| Carbon steel heat exchanger shells in refinery service | Hydrogen damage near and away from welds [5] | Total focusing method and low-angle time-of-flight diffraction; velocity ratio missed thin damage [5] | [Conventional UT vs phased array (PAUT) vs time-of-flight diffraction (TOFD)](/library/ut-vs-paut-vs-tofd/) |
| Plate and pipe body with inclusions | Hydrogen uptake from sour water; no stress needed [1] | Ultrasonic testing for in-plane cracks; visual check for blisters [2][5] | [Hydrogen induced cracking](/glossary/hydrogen-induced-cracking/) |

Sources: NBSIR 86-3049 [4]; NIST SP 780 [2]; OSHA Technical Manual [3]; Kaley and others, 1996 [8]; Kazys and others, 2022 [5]; Martin and Sofronis, 2022 [1].

## Sources

1. [Hydrogen-Induced Cracking and Blistering in Steels: A Review (M. L. Martin and P. Sofronis), Journal of Natural Gas Science and Engineering 101, 104547, US National Institute of Standards and Technology (NIST)](https://www.nist.gov/publications/hydrogen-induced-cracking-and-blistering-steels-review), 2022-03-31
2. [NIST Special Publication 780, Guidelines for Pressure Vessel Safety Assessment (S. Yukawa), US National Institute of Standards and Technology (NIST)](https://nvlpubs.nist.gov/nistpubs/Legacy/SP/nistspecialpublication780.pdf)
3. [OSHA Technical Manual, Section IV, Chapter 3: Pressure Vessel Guidelines, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-3)
4. [NBSIR 86-3049, Examination of a Pressure Vessel that Ruptured at the Chicago Refinery of the Union Oil Company on July 23, 1984 (H. I. McHenry and others), US National Bureau of Standards (now NIST)](https://nvlpubs.nist.gov/nistpubs/Legacy/IR/nbsir86-3049.pdf)
5. [Comparative Analysis of Ultrasonic NDT Techniques for the Detection and Characterisation of Hydrogen-Induced Cracking (R. J. Kazys, L. Mazeika, V. Samaitis, R. Sliteris, P. Merck, Z. Viliunas), Materials 15(13):4551, MDPI, via PubMed Central (open access, CC BY 4.0)](https://pmc.ncbi.nlm.nih.gov/articles/PMC9267232/), 2022-06-28
6. [30 CFR 250.490, Hydrogen sulfide, Electronic Code of Federal Regulations (eCFR)](https://www.ecfr.gov/current/title-30/section-250.490)
7. [A Review of the Factors That Can Increase the Risk of Sulfide Stress Cracking in Thermomechanical Controlled Processed Pipeline Steels (S. Hiew Sze Kei, W. M. van Haaften, T. B. Britton, S. Pedrazzini), Advanced Engineering Materials 25(21), Imperial College London repository (open access, CC BY)](https://spiral.imperial.ac.uk/entities/publication/954bf13b-a5a8-4ccf-a67c-2457d297c96e)
8. [Research report on ultrasonic characterization and monitoring of cracking in wet H2S service (L. C. Kaley, K. C. Van Scyoc, M. Prager, M. S. Cayard, R. D. Kane), OSTI record 403561, US Department of Energy, Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/403561)
9. [Potentially Hazardous Amine Absorber Pressure Vessels Used in Refinery Processing (standard interpretation memorandum), US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/laws-regs/standardinterpretations/1986-04-11), 1986-04-11

Published by Winda Beacon (https://beacon.winda.ai).