# What is high temperature hydrogen attack (HTHA)?

> High temperature hydrogen attack (HTHA) is damage to carbon and low-alloy steel exposed to hot, high-pressure hydrogen. Hydrogen enters the steel and reacts with its carbon to form methane, which cannot escape and opens fissures and cracks. API RP 941 is the industry practice for choosing steels for this service.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T09:39:01+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: Refining
- Canonical: https://beacon.winda.ai/library/high-temperature-hydrogen-attack/

## Why does it matter?

The carbon steel heat exchanger that ruptured from HTHA at a refinery in Anacortes, Washington, on April 2, 2010, was estimated by the US Chemical Safety and Hazard Investigation Board (CSB) to have operated below the industry curve treated as the safe limit [1]. Hydrogen and naphtha hotter than 500 °F (about 260 °C) escaped and ignited, and seven workers died [1]. The CSB concluded that the carbon steel curve cannot be relied on to predict HTHA, and noted in 2016 that the new edition of the industry practice listed 13 more failures below it [1][2].

## How does HTHA damage steel?

Hydrogen molecules split into atoms at the hot steel surface, and the atoms diffuse into the wall [1]. Inside, hydrogen reacts with carbon in the steel to form methane, which strips carbon from the metal (decarburization) [1]. Methane molecules are too large to diffuse back out, so they collect inside the steel and build pressure [1][5].

That pressure opens small fissures and blisters, which join into microcracks and then larger cracks until the weakened wall can rupture, as at Anacortes [1]. Steels alloyed with chromium and molybdenum hold their carbon in more stable carbides, so they resist HTHA to higher temperatures and hydrogen pressures than plain carbon steel [1].

## What makes equipment susceptible?

- **Temperature and hydrogen partial pressure.** For a given steel, higher temperature makes HTHA more likely [1]. Hydrogen partial pressure is the share of the total gas pressure that comes from hydrogen [1].
- **Welds and residual stress.** Damage collects in high-stress areas such as welds that were not post-weld heat treated (PWHT); at Anacortes, HTHA was found only near such welds [1]. PWHT gives a modest improvement [1].
- **Actual versus design conditions.** Damage mechanism reviews at Anacortes over 20 years relied on design data, so the exchangers were never inspected for HTHA; the CSB's modeling estimated that the hottest section at times ran above the carbon steel curve [1].
- **Cladding.** Stainless steel cladding lowers the effective hydrogen partial pressure on the carbon steel beneath it. At Anacortes only the hottest of four shell sections was clad, while review documents listed the whole shell as clad [1].

## How are operating limits for HTHA set?

The industry reference is API Recommended Practice (RP) 941, *Steels for Hydrogen Service at Elevated Temperatures and Pressures in Petroleum Refineries and Petrochemical Plants*, first published in 1970 [1][3]. It contains operating-limit curves, known as Nelson curves, for carbon steel and chromium-molybdenum steels plotted against temperature and hydrogen partial pressure [3]. The curves go back to George Nelson's 1949 work and are revised as companies report new cases; the CSB found the reported process data ill-defined and inconsistent [1]. Beacon does not reproduce the curves.

API's 2025 catalog lists the 8th edition (February 2016), whose carbon steel curves are split into equipment with and without PWHT [2][3]. API RP 571, on damage mechanisms in refinery equipment, names steels not susceptible to HTHA at normal refinery conditions [2].

## How is HTHA found?

With difficulty. The CSB found that early damage can be microscopic and local, and that success depends on technique and on inspector skill few people have [1]. It concluded that inspection alone is not reliable enough to control HTHA [1][2].

- **Advanced ultrasonic backscatter.** The best method available in 2014, according to the CSB, but it needs a very high level of expertise and has no general inspector certification [1].
- **Velocity ratio.** HTHA slows longitudinal sound waves slightly more than shear waves; the CSB reports the ratio works only at high damage levels and in base metal [1]. In a 2022 laboratory comparison on hydrogen-damaged steel from a refinery exchanger, it found nothing where the damaged layer was thin [5].
- **Newer ultrasonic imaging.** The same study found total focusing method imaging resolved cracks close to 0.2 mm, and a low-angle time-of-flight diffraction probe suited screening of large areas [5].

In 2018 the UK Health and Safety Executive (HSE) published two research reports on HTHA: one on non-destructive testing techniques, one on factors affecting carbon steels [4].

## What did investigators recommend?

The CSB concluded that inherently safer materials are a better defense than inspection or PWHT, which depend on procedures and people [1]. It recommended that API revise RP 941 to set minimum requirements, require inherently safer materials where feasible, require verification of actual operating conditions, and prohibit carbon steel above 400 °F (204 °C) and 50 psia hydrogen partial pressure [2]. These limits are the CSB's own recommendation, not API values. In July 2016 the CSB judged API's response unacceptable and issued guidance to replace such carbon steel with higher chromium-molybdenum steels [2].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Carbon steel heat exchangers in hydrotreating and reforming | Hot, high-pressure hydrogen-rich streams; above 500 °F (about 260 °C) at Anacortes [1] | Specialized ultrasonic methods such as backscatter; results depend on inspector skill [1] | [What is hydroprocessing (hydrotreating and hydrocracking)?](/library/hydroprocessing/) |
| Welds and heat-affected zones without PWHT | Residual stress concentrates damage; Anacortes damage was found only near welds [1] | Ultrasonic imaging at welds, such as phased array, tried for HTHA in research; early damage is hard to find [1][5] | [Phased array ultrasonic testing](/glossary/phased-array-ultrasonic-testing/) |
| Equipment whose steel was chosen from design data | Actual temperatures above design, with little instrumentation [1] | Comparing measured temperature and hydrogen partial pressure with the steel's limits [1][2] | [What are integrity operating windows (IOWs)?](/library/integrity-operating-windows/) |
| Base metal with advanced damage | Fissures linked into cracks [1] | Velocity ratio, at high damage levels only; imaging methods under study [1][5] | What are the main non-destructive testing (NDT) methods in oil and gas? |
| Stainless-clad carbon steel shells | Cladding protects only the steel it covers; records may overstate its extent [1] | Checking fabrication records against the actual clad sections [1] | What is a damage mechanism review? |

Sources: CSB Report 2010-08-I-WA, 2014 [1]; CSB Safety Alert on HTHA, 2016 [2]; Kazys and others, Materials, 2022 [5].

## Sources

1. [Investigation Report: Catastrophic Rupture of Heat Exchanger (Seven Fatalities), Tesoro Anacortes Refinery, Anacortes, Washington, April 2, 2010 (Report 2010-08-I-WA), US Chemical Safety and Hazard Investigation Board (CSB)](https://www.csb.gov/assets/1/6/Tesoro_Anacortes_2014-May-01.pdf?15244)
2. [CSB Safety Alert: Preventing High Temperature Hydrogen Attack (HTHA), US Chemical Safety and Hazard Investigation Board (CSB)](https://www.csb.gov/assets/1/20/Safety_Alert_HTHA_Final1.pdf?16371)
3. [2025 Publications Catalog (entries for RP 941 and TR 941-A) (RP 941, 8th edition, February 2016; TR 941-A, 1st edition, September 2008), American Petroleum Institute (API)](https://www.api.org/-/media/files/publications/2025-catalog/2025_pubs%20catalog.pdf)
4. [Research reports 1101 to 1200 (index listing RR1133 and RR1134 on high temperature hydrogen attack), UK Health and Safety Executive (HSE)](https://www.hse.gov.uk/research/rrhtm/1101-1200.htm)
5. [Comparative Analysis of Ultrasonic NDT Techniques for the Detection and Characterisation of Hydrogen-Induced Cracking (R. J. Kazys, L. Mazeika, V. Samaitis, R. Sliteris, P. Merck, Z. Viliunas), Materials 15(13):4551, MDPI, via PubMed Central (open access, CC BY 4.0)](https://pmc.ncbi.nlm.nih.gov/articles/PMC9267232/), 2022-06-28

Published by Winda Beacon (https://beacon.winda.ai).