# What is high-temperature oxidation?

> High-temperature oxidation is the reaction of a metal with oxygen in hot air, flue gas or steam, which grows an oxide scale on its surface. A thin, adherent scale slows further attack; thick or flaking scale thins the wall and hinders heat transfer. Alloys richer in chromium form more protective scales.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T09:39:01+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: Refining
- Canonical: https://beacon.winda.ai/library/high-temperature-oxidation/

## Why does it matter?

A 2014 model from Oak Ridge National Laboratory (ORNL) predicted that oxide scale flaking from the steam side of stainless steel superheater tubes could block more than half of a tube bend within the first two years of boiler operation, at outlet tube temperatures of 540 to 570 °C (about 1,000 to 1,060 °F) [3]. The authors noted that this matched practical experience [3]. A blocked tube is starved of steam and can overheat: boiler failure reports reviewed by Basson and Fuls (2021) found short-term overheating caused by oxide scaling most often in horizontal superheaters [6]. A thin, adherent scale protects the metal; the problems start when scale grows thick or breaks away [1][2].

## How does a metal oxidize at high temperature?

When hot metal meets oxygen, the two react at the surface and build a solid oxide layer, called scale [1][2]. Once the scale covers the surface, the reaction can continue only as metal or oxygen ions move through it, so the scale itself sets the pace [2]. Most cases follow one of three rate laws: linear, where the rate stays constant because a surface reaction, not the scale, controls it; parabolic, where growth slows with time because diffusion through a thickening scale controls it; and logarithmic, which applies to very thin films [2].

Temperature has a strong effect. The UK National Physical Laboratory (NPL) gives a rule of thumb that, for many oxidation reactions, a change of 20 °C (36 °F) changes the oxidation rate about tenfold [1]. Polluted hot gases, such as sulfur oxides, chlorine compounds and nitrogen oxides, can speed the attack further [1].

## Which metals resist it?

Resistance rises with chromium, which helps form a tight, adherent chromium oxide scale [4]. Work at Argonne National Laboratory (ANL) in hot, carbon-rich reformer gas found chromium oxide the most protective scale on commercial alloys [5].

NPL's checklist gives approximate temperatures below which oxidation in air is negligible: about 480 °C (about 900 °F) for mild steel, about 900 °C (about 1,650 °F) for grade 316 stainless steel and about 1,150 °C (about 2,100 °F) for a 25% chromium, 20% nickel stainless steel [1]. NPL adds that creep strength or polluted gases can set lower practical limits [1]; see [What is creep damage?](/library/creep/).

## What damage does it cause?

- **Metal loss.** Scale grows by consuming metal, so the wall gets thinner [1][2].
- **Overheating.** Scale and deposits slow heat transfer more as they thicken, and NPL notes that thick scale and metal loss lead to overheating when tubes lose their cooling [1].
- **Spalling and blockage.** Oxide takes up more volume than the metal it replaces, which stresses the scale; in laboratory tests the scale on pure iron ballooned and separated from the metal on cooling [2]. ORNL modeling predicted that the earliest scale failures in superheater tubes would come from strains during boiler shutdowns, and the flakes can block tube bends [7][3].
- **Opening the way to other damage.** In ethylene cracking tubes, carburization starts where the oxide scale spalls [4]. In steam reformer tubes, oxidation of the inner surface changes thermal stress and creep damage [8].

## How is it found?

- **Thickness, dimensions and surface condition.** A 1994 field method for ethylene furnace tubes combined dimension and thickness measurements, visual inspection and surface replicas with electromagnetic instruments to assess oxidation and carburization together [9].
- **Prediction for steam-side scale.** ORNL's models estimate scale growth, flaking and the share of a tube bend likely to be blocked, as a function of operating time and steam temperature [3][7].
- **After a failure.** Blockage often comes to light when a tube overheats and ruptures [6]; see [What is short-term overheating of heater tubes?](/library/short-term-overheating/).

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Boiler superheater and reheater tubes | Steam-side scale grows, then flakes during shutdowns and collects in bends [3][7] | Scale growth and blockage modeling; often found after a tube overheats [3][6] | [What is short-term overheating of heater tubes?](/library/short-term-overheating/) |
| Ethylene cracking furnace tubes | Oxidation alongside carburization at very high wall temperatures [9] | Thickness and dimension checks, visual inspection, replicas and electromagnetic surveys [9] | [What is a petrochemical plant?](/library/petrochemical-plant/) |
| Cast heat-resistant coils where scale spalls | Bare metal exposed to carbon-rich process gas [4] | Magnetic response of carburized metal [4] | What is carburization? |
| Steam reformer tubes | Inner-surface oxidation changes thermal stress and creep [8] | Full-length eddy current with laser deformation measurement [8] | [What is creep damage?](/library/creep/) |
| Tubes heated by hot gas | Thick scale and metal loss raise metal temperature [1] | Wall thickness measurement [9] | [How does ultrasonic thickness measurement work?](/library/ultrasonic-thickness-measurement/) |

Sources: NPL, 2020 [1]; ORNL, 2011 and 2014 [3][7]; Saori and Ohta [4]; Basson and Fuls, 2021 [6]; HIAD record of the 2018 KHK case [8]; Lin and others, 1994 [9].

## Sources

1. [Corrosion control checklist (Guides to Good Practice in Corrosion Control No. 11), UK National Physical Laboratory (NPL)](https://eprintspublications.npl.co.uk/8621/)
2. [High-Temperature Oxidation of Metals (S. Samal), book chapter, DOI 10.5772/63000, IntechOpen (open access)](https://www.intechopen.com/chapters/50691), 2016-09-07
3. [Managing Oxide Scale Exfoliation in Boilers with TP347H Superheater Tubes (A. S. Sabau, I. G. Wright, J. P. Shingledecker, P. F. Tortorelli), conference paper (record and abstract), Oak Ridge National Laboratory, via US DOE Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/1126527)
4. [Carburization and its prevention in ethylene cracking furnace tubes (M. Saori, S. Ohta), TMS Paper Selection vol. 56 (record and abstract), US DOE Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/5393467)
5. [Argonne National Laboratory Develops Alloys to Resist Metal Dusting (fact sheet), US Department of Energy, Industrial Technologies Program](https://www1.eere.energy.gov/manufacturing/industries_technologies/imf/pdfs/metaldusting.pdf)
6. [Over-attemperation and Short-term Overheating in Pendant-type Superheaters (N. Basson, W. F. Fuls), R&D Journal of the South African Institution of Mechanical Engineering 37, 58-69, South African Institution of Mechanical Engineering (open access, CC BY 4.0)](https://rdj.journals.ac.za/index.php/pub/article/view/21)
7. [Steam-Side Oxide Scale Exfoliation Behavior in Superheaters and Reheaters (A. S. Sabau, J. P. Shingledecker, I. G. Wright), conference paper (record and abstract), Oak Ridge National Laboratory, via US DOE Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/1037623)
8. [Process gases leak in a reformer tube (HIAD 2.0 incident record, based on KHK accident database incident 2018-428), Clean Hydrogen Partnership, Clean Hydrogen Knowledge Hub (European Union)](https://knowledge.clean-hydrogen.europa.eu/hiad/incidents/process-gases-leak-reformer-tube)
9. [The field measurement of carburization and oxidation of ethylene furnace tubes by multi-technique method (J. Y. Lin, F. C. Chiang, H. Chang, C. C. Su) (record and abstract), US DOE Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/70110)