# What is hydrogen embrittlement?

> Hydrogen embrittlement is the loss of ductility, toughness or fatigue resistance in a metal after hydrogen atoms enter it. The metal can then crack at stresses it would normally carry. Hydrogen comes from corrosion, cathodic protection, electroplating or hydrogen gas, and high-strength steels are especially susceptible. ASME B31.12 covers hydrogen piping and pipelines.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T09:39:01+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: Pipelines, Refining, Upstream and offshore
- Canonical: https://beacon.winda.ai/library/hydrogen-embrittlement/

## Why does it matter?

On December 18, 2012, in the Gulf of Mexico, the bolts holding a drilling rig's lower marine riser package to its blowout preventer stack broke, the two separated, and about 432 barrels of synthetic-based drilling fluid were released [1]. The US Bureau of Safety and Environmental Enforcement (BSEE) found that the bolts failed mainly by hydrogen-induced stress corrosion cracking caused by hydrogen embrittlement [1]. More than 10,000 bolts were replaced within a short period, and BSEE noted that a 2003 riser bolt failure had already raised concerns about hardness and cathodic protection [1].

## How does hydrogen embrittle a metal?

Hydrogen is the smallest atom, so it can settle on a metal surface, diffuse inside and collect unevenly at features of the microstructure, lowering strength, ductility and fracture toughness [2]. A 2024 review describes the problem as three factors acting together: load, a source of hydrogen and a susceptible material [2]. Theories from the 1970s include hydrogen weakening the bonds between atoms (hydrogen-enhanced decohesion) and hydrogen easing local plastic flow (hydrogen-enhanced localized plasticity); recent work suggests several mechanisms act together, and the debate continues [2].

The damage can be invisible. The US National Institute of Standards and Technology (NIST) notes that dissolved hydrogen lowers ductility and fracture toughness without creating internal flaws [7]. As hydrogen content rises, fracture surfaces change from ductile dimples to flatter quasi-cleavage and sometimes intergranular facets [2].

## Where does the hydrogen come from?

- **Manufacturing.** Hydrogen can enter during casting, heat treatment or electroplating; trapped under a coating it can cause delayed fracture, so parts are often baked at low temperature to drive it out [2]. The 2012 bolts had not received the post-plating bake that the plating specification required [1].
- **Corrosion.** Corrosion in water containing hydrogen sulfide (H2S) is a prime example of a reaction that pushes hydrogen into carbon and low-alloy steel [7]. US offshore rules note that sulfide stress cracking is also known as hydrogen embrittlement (30 CFR 250.490(p)) [9].
- **Cathodic protection.** The more negative the protection potential, the more hydrogen the steel can absorb, and unpainted areas draw more current [1].
- **Hydrogen gas.** Pipelines and pressure vessels carrying hydrogen expose steel and welds directly [3][5].

## Which materials are most susceptible?

- **High-strength steels.** The National Aeronautics and Space Administration (NASA) lists high-strength steels and titanium among the metals affected, and the 2024 review notes that the problem usually grows with alloy strength [2][6]. The failed subsea bolts were specified at 34 to 38 on the Rockwell C hardness scale, and BSEE concluded that hardness above 34 in subsea service remains an issue [1].
- **Almost every alloy used for hydrogen.** Ferritic and austenitic stainless steels, nickel, aluminium and titanium alloys are all affected to some degree [2]. In one example in the review, hydrogen cut a pipeline steel's ultimate strength by over 50% and its ductility by over 90% [2].
- **Carbon steel already charged with hydrogen.** In the 1984 refinery amine absorber investigated by the National Bureau of Standards (NBS), hydrogen had lowered the steel's toughness enough for an 800 mm crack to break the vessel at its normal operating stress of 35 MPa (5.1 ksi) [8].

## What does it mean for hydrogen pipelines?

The US Department of Energy (DOE), on a page updated in June 2026, reports about 1,600 miles of hydrogen pipelines operating in the United States, near large users such as refineries and chemical plants on the Gulf Coast, and lists embrittlement of pipeline steel and welds as a research concern [5]. DOE adds that blending up to about 15% hydrogen into natural gas pipelines may need only modest changes, while pure hydrogen may need more [5].

Fatigue matters more than tensile ductility here. NIST points out that pipelines run well below yield, most ductility loss appears only after peak strength, and pipelines used for storage may see two to three pressure cycles a day [3]. In NIST tests in hydrogen gas at 5.5 and 34 MPa, fatigue cracks in pipeline welds, heat-affected zones and base metal grew at least 10 times faster than in air over much of the tested range [3]. NIST led a change to ASME B31.12 that permits X70 pipe steel rather than X52 [4].

## How is it found and controlled?

Hydrogen can weaken steel without creating any internal flaw, so there may be nothing for inspection to find until a crack forms [7]. In the cases on this page it was identified after fracture: NASA's laboratory found intergranular cleavage on a broken plated spring, the 1984 vessel was explained by toughness tests on hydrogen-charged samples, and the 2012 bolts by a root cause analysis that BSEE reviewed [1][6][8].

Controls described in public sources include baking parts after plating, lower hardness and strength for subsea bolting, consistent hardness guidance across standards, limits on cathodic protection voltage, and testing materials in hydrogen before use [1][2][3][6]. BSEE also called for industry failure reporting so that problems like the 2003 and 2012 bolt failures are shared [1]. For hot hydrogen service, API's catalog notes that rapid cooling after high-temperature, high-pressure operation may require outgassing of hydroprocessing reactors, a topic outside its practice on high temperature hydrogen attack (HTHA) [11].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Subsea connector bolts on drilling risers and blowout preventer stacks | Hard alloy steel bolts; electroplating without the required bake; cathodic protection [1] | Fracture in service, then root cause analysis and regulator review [1] | How does cathodic protection work? |
| Electroplated high-strength springs and fasteners | Plating hydrogen not baked out [6] | Electron microscope fractography showing intergranular cleavage [6] | How are materials selected for oil and gas equipment? |
| Hydrogen and blended gas pipelines, including welds | Pressure cycling in hydrogen gas [3][5] | Fatigue crack growth testing in pressurized hydrogen, at least 10 times faster than in air [3] | Can existing gas pipelines carry hydrogen? |
| Carbon steel vessels in wet H2S service | Hydrogen from sour corrosion; blisters and delamination show it is entering [7][8] | Visual blisters, ultrasonic delamination checks, and toughness tests on hydrogen-charged samples after failure [7][8] | What is wet hydrogen sulfide (H2S) damage? |

Sources: BSEE QC-FIT Report 2014-01 [1]; NASA KSC [6]; Drexler and others (NIST), 2019 [3]; DOE [5]; NIST SP 780 [7]; NBSIR 86-3049 [8].

## Sources

1. [QC-FIT Evaluation of Connector and Bolt Failures, Summary of Findings, QC-FIT Report #2014-01, US Bureau of Safety and Environmental Enforcement (BSEE)](https://www.bsee.gov/sites/bsee.gov/files/reports/drilling/bolt-report-final-8-4-14.pdf)
2. [Hydrogen Embrittlement as a Conspicuous Material Challenge: Comprehensive Review and Future Directions (H. Yu and others), Chemical Reviews 124(10):6271-6392, American Chemical Society, via PubMed Central (open access, CC BY 4.0)](https://pmc.ncbi.nlm.nih.gov/articles/PMC11117190/), 2024-05-09
3. [Fatigue Testing of Pipeline Welds and Heat-Affected Zones in Pressurized Hydrogen Gas (E. S. Drexler and others), Journal of Research of NIST 124:124008, US National Institute of Standards and Technology (NIST)](https://nvlpubs.nist.gov/nistpubs/jres/124/jres.124.008.pdf), 2019-04-26
4. [Materials Testing in Extreme Environments (project page), US National Institute of Standards and Technology (NIST)](https://www.nist.gov/programs-projects/materials-testing-extreme-environments)
5. [Hydrogen Pipelines, US Department of Energy (DOE), Hydrogen and Fuel Cell Technologies Office](https://www.energy.gov/eere/fuelcells/hydrogen-pipelines)
6. [Forms of Corrosion, NASA Kennedy Space Center (KSC), Corrosion website](https://public.ksc.nasa.gov/corrosion/forms-of-corrosion/)
7. [NIST Special Publication 780, Guidelines for Pressure Vessel Safety Assessment (S. Yukawa), US National Institute of Standards and Technology (NIST)](https://nvlpubs.nist.gov/nistpubs/Legacy/SP/nistspecialpublication780.pdf)
8. [NBSIR 86-3049, Examination of a Pressure Vessel that Ruptured at the Chicago Refinery of the Union Oil Company on July 23, 1984 (H. I. McHenry and others), US National Bureau of Standards (now NIST)](https://nvlpubs.nist.gov/nistpubs/Legacy/IR/nbsir86-3049.pdf)
9. [30 CFR 250.490, Hydrogen sulfide, Electronic Code of Federal Regulations (eCFR)](https://www.ecfr.gov/current/title-30/section-250.490)
10. [Hydrogen-Induced Cracking and Blistering in Steels: A Review (M. L. Martin and P. Sofronis), Journal of Natural Gas Science and Engineering 101, 104547, US National Institute of Standards and Technology (NIST)](https://www.nist.gov/publications/hydrogen-induced-cracking-and-blistering-steels-review), 2022-03-31
11. [2025 Publications Catalog (entry for RP 941) (RP 941, 8th edition, February 2016), American Petroleum Institute (API)](https://www.api.org/-/media/files/publications/2025-catalog/2025_pubs%20catalog.pdf)

Published by Winda Beacon (https://beacon.winda.ai).