# What is intergranular corrosion?

> Intergranular corrosion is attack along or beside the grain boundaries of a metal while the grains themselves corrode little. In austenitic stainless steel it usually follows sensitization, when heat from welding or service forms chromium carbides at the boundaries and leaves chromium-poor zones. ASTM A262 sets laboratory tests for susceptibility.

- Label: Fact
- Type: Explainer
- Published: 2026-11-14T11:57:56+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-14
- Topics: LNG, Refining
- Canonical: https://beacon.winda.ai/library/intergranular-corrosion/

## Why does it matter?

Welding can leave austenitic stainless steel corroding in a band a short distance from the weld, while the weld itself and the rest of the plate stay sound; the National Aeronautics and Space Administration (NASA) describes this as the typical pattern in these steels [1]. Because the attack follows narrow paths between grains, it can weaken metal badly, and in severe cases whole grains fall out [2]. Under stress the same weakness becomes intergranular stress corrosion cracking: in 1988 the US Nuclear Regulatory Commission (NRC) reported that inspections had found significant numbers of cracked welds in stainless reactor piping at almost all operating boiling water reactors [5].

## How does intergranular corrosion happen?

A metal is made of many small crystals (grains), and the boundaries between them differ chemically from the grain interiors [1]. Impurities can gather at the boundaries, or new phases can form there [2]. If the zone next to a boundary loses an element it needs to resist corrosion, that zone becomes anodic to the rest of the surface and corrodes first, along a narrow path [2].

In austenitic stainless steel the element lost is chromium. When carbon combines with chromium to form carbides at the boundaries, the thin band beside them is left with too little chromium to keep its protective passive film [3].

## When does stainless steel become sensitized?

- **In a temperature window.** A 2026 review places carbide formation between about 400 and 900 °C (750 to 1,650 °F) and finds that steels sensitize once held long enough at about 500 to 800 °C, with the exact threshold depending on composition [3].
- **During welding.** The heat-affected zone passes through this range; reheating by later passes in multipass welding is a common cause [2].
- **In service, even below the nominal range.** Stabilized 347 furnace tubes overheated to 512 °C under coke deposits and cracked along grain boundaries, and 347H tubing showed intergranular attack after 25 years at 270 to 310 °C [3]. In a 2002 refinery case the process stream ran at 330 °C, which seemed too cool to sensitize the tubes, but the tube metal in the fired heater was about 405 °C [7].
- **Deliberately, for testing.** US tank car rules require 304L and 316L test pieces to receive a sensitizing treatment, typically 1 hour at 1,250 °F (about 677 °C), before the intergranular attack test in ASTM A262 (49 CFR 179.200-7(d)) [4].

## Which alloys are affected?

- **Austenitic stainless steels.** Low-carbon grades such as 304L and 316L, and grades stabilized with titanium or niobium such as 321 and 347, resist sensitization in normal welding [1][9].
- **Stabilized grades are not immune.** Stabilization delays carbide formation but may not suffice at higher temperatures, especially in welds [3]. A narrow form called knife-line attack occurs right next to the weld in stabilized grades [2], and a hydrocracker's 347 furnace tubes became sensitized through local overheating [8].
- **Other austenitic alloys.** Polythionic acid cracking also affects sensitized austenitic alloys other than stainless steel [9].
- **Aluminium alloys.** Heat-treatable 2000, 6000 and 7000 series alloys are prone, and exfoliation, a form that lifts layers of grains, is common in extrusions; it can also occur on carbon steel [1][2].

## What forms does it take in oil and gas equipment?

- **Weld decay**, the band of attack in the heat-affected zone [1][2].
- **Polythionic acid stress corrosion cracking**, intergranular cracking of sensitized stainless steel when sulfide scale meets air and moisture during shutdowns; a naphtha hydrotreater heater coil cracked this way after about 18 years in service [7][9].
- **Chloride cracking of sensitized steel.** Type 321 heater tubes in heavy crude service failed by intergranular cracking attributed to chlorides at about 130 to 345 °C [3].

## How is it found?

- **Laboratory etch tests.** Etching a polished sample in oxalic acid, Practice A of ASTM A262, showed wide "ditched" grain boundaries that marked the 2002 heater tubes as sensitized [7].
- **Field electrochemical tests.** A double-loop electrochemical potentiokinetic reactivation (DL-EPR) test with a portable cell was used without cutting samples across the heat-affected zone of a welded 304 tube; the readings showed the most sensitization next to the weld bead [6]. The same test confirmed sensitization in the failed 347 tubes [8].
- **Metallography and fractography** of cracked sections show whether the path runs between grains [7].
- **Inspection programs targeted by susceptibility.** The NRC set inspection schedules for stainless reactor piping welds according to their susceptibility and mitigation [5].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Heat-affected zones of austenitic stainless welds | Weld heat and reheating by later passes form chromium carbides [1][2] | Portable DL-EPR readings on the weld zone; oxalic acid etch on samples [6][7] | [What are a welding procedure specification (WPS) and a procedure qualification record (PQR)?](/library/welding-procedure-specification/) |
| Stainless heater tubes in hydrotreaters and hydrocrackers | Tube metal hotter than the process; local overheating under coke [7][8] | Cracks found after shutdown; microstructure and DL-EPR confirmed sensitization [7][8] | [What is a fired heater?](/library/fired-heater/) |
| Hydroprocessing equipment opened during shutdowns | Sensitized steel, sulfide scale, air and moisture [7][9] | Metallography and fractography showing an intergranular path [7] | [What is polythionic acid stress corrosion cracking?](/library/polythionic-acid-scc/) |
| Stainless heater tubes in heavy crude service | Chlorides at about 130 to 345 °C [3] | Failure analysis showing intergranular cracking [3] | [What is chloride stress corrosion cracking?](/library/chloride-stress-corrosion-cracking/) |
| Stainless reactor piping welds (nuclear record, outside oil and gas) | Intergranular stress corrosion cracking near welds [5] | Extensive inspection programs found cracked welds at almost all operating boiling water reactors [5] | [What should an inspection plan contain?](/library/inspection-plan/) |

Sources: NASA KSC [1]; AMPP [2]; Ardila-Parra and others, 2026 [3]; NRC Generic Letter 88-01 [5]; Caetano and others, 2012 [6]; Lobley, 2002 [7]; Swaminathan and others, 2011 [8]; AFPM, 2016 [9].

## Sources

1. [Forms of Corrosion, NASA Kennedy Space Center (KSC), Corrosion website](https://public.ksc.nasa.gov/corrosion/forms-of-corrosion/)
2. [Intergranular Corrosion, Association for Materials Protection and Performance (AMPP)](https://ampp.org/technical-research/impact/intergranular-corrosion)
3. [Understanding failure in austenitic steels: Key considerations for molten salt storage in CSP applications (S. A. Ardila-Parra, C. Prieto, J. D. Osorio, A. I. Fernández), Journal of Materials Research and Technology 41, US Department of Energy, Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/servlets/purl/3027701)
4. [49 CFR 179.200-7, Materials (tank cars), Electronic Code of Federal Regulations (eCFR)](https://www.ecfr.gov/current/title-49/section-179.200-7)
5. [NRC Position on IGSCC in BWR Austenitic Stainless Steel Piping (Generic Letter No. 88-01), US Nuclear Regulatory Commission (NRC)](https://www.nrc.gov/reading-rm/doc-collections/gen-comm/gen-letters/1988/gl88001.html), 1988-01-25
6. [Análise da Susceptibilidade à Corrosão Localizada de um Tubo Soldado de Aço AISI 304 Pela Técnica Eletroquímica de Reativação Potenciocinética Cíclica (EPR-DL) (G. de Q. Caetano and others), INTERCORR 2012, paper 259, Associação Brasileira de Corrosão (ABRACO)](https://abraco.org.br/src/uploads/intercorr/2012/INTERCORR2012_259.pdf)
7. [Stress Corrosion Cracking: Case Studies in Refinery Equipment (G. R. Lobley), 6th Saudi Engineering Conference, Vol. 5, King Fahd University of Petroleum and Minerals (KFUPM), conference proceedings](https://faculty.kfupm.edu.sa/coe/sadiq/proceedings/SEC2002/vol5/P017.pdf)
8. [Sensitization induced stress corrosion failure of AISI 347 stainless steel fractionator furnace tubes (J. Swaminathan, R. Singh, M. K. Gunjan, B. Mahato), Engineering Failure Analysis 18(8), CSIR-National Metallurgical Laboratory (NML), Eprints@NML (abstract)](https://eprints.nmlindia.org/4222)
9. [Q&A, Question 20: When is it appropriate to neutralize austenitic stainless-steel equipment to protect against stress corrosion cracking?, American Fuel & Petrochemical Manufacturers (AFPM)](https://afpm.org/print/pdf/node/42154)

Published by Winda Beacon (https://beacon.winda.ai).