# What is naphthenic acid corrosion?

> Naphthenic acid corrosion (NAC) is metal loss caused by organic acids that occur naturally in some crude oils, attacking steel in hot oil. It is reported at roughly 220 to 400 °C (430 to 750 °F) in crude and vacuum distillation units, is worst where flow is fast or acids condense, and leaves sharp-edged pits and grooves.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T15:24:40+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: Refining
- Canonical: https://beacon.winda.ai/library/naphthenic-acid-corrosion/

## Why does it matter?

The chromium steels that slow sulfidation do not reliably stop naphthenic acid corrosion. A 2008 paper reviewing refinery experience found that moving from carbon steel through 5Cr, 9Cr and 12Cr steels did little in severe NAC service, and that upgrading to molybdenum-bearing 316 stainless steel was needed [3]. Laboratory data in the same paper show corrosion falling as molybdenum content rises [3]. So a unit built for high-sulfur crude is not necessarily protected when it starts processing more acidic crude [3][4].

## What causes naphthenic acid corrosion?

In the industry, "naphthenic acid" refers collectively to all the organic (carboxylic) acids in crude oil [3]. NAC was first seen in the 1920s in crude distillation in Romania, Azerbaijan, Venezuela and California [3], and a 1986 review lists acidic crudes from India, Russia, Texas, Congo and Nigeria among others [2].

The acids react directly with iron in the hot oil. Crude oil barely conducts electricity, so this is a chemical reaction rather than the electrochemical corrosion seen in water [4]. The corrosion products dissolve in the oil, which is why NAC typically leaves a bare, scale-free surface [3][4].

Acid content is measured as the total acid number (TAN): the milligrams of potassium hydroxide needed to neutralize the acid in one gram of oil, by ASTM D664 (potentiometric) or ASTM D974 (color indicator) titration [3][4].

## What controls the corrosion rate?

- **Temperature.** Damage is reported from about 220 to 400 °C (430 to 750 °F); above about 400 °C it is usually not seen, probably because the acids break down or a protective coke film forms [2][3]. OSHA notes that naphthenic acids can become corrosive above 450 °F (about 230 °C) when the crude's acid value is above a certain level [1].
- **Acid content.** Corrosion rises once the acid number passes a certain level [2]. Acid number alone does not predict corrosion, because process conditions, materials and crude blends differ from unit to unit [3].
- **Velocity and phase change.** High velocity, turbulence and wall shear stress speed up NAC, especially in two-phase flow, and attack is often worst where acids vaporize or condense [3].
- **Sulfur.** Sulfur compounds interact with NAC. Iron sulfide scale can protect the steel, but hydrogen sulfide can also convert dissolved iron naphthenate to iron sulfide and free the acid again [3]. Under refinery conditions, NAC and sulfidation usually proceed together [4].
- **Alloy.** Chromium alone helps little; molybdenum-bearing austenitic stainless steels such as 316 and 317 resist NAC better [3].

## Where does it occur in a refinery?

The 2008 paper describes three typical environments [3]:

- **Furnace tubes and transfer lines** of atmospheric and vacuum units, where attack depends on velocity and vaporization. [3]
- **Vacuum columns**, in the light and heavy vacuum gas oil sections, where acids condense near their boiling range; here attack depends on acid content more than velocity. [3]
- **Side-cut piping**, where attack depends on acid content and is partly held back by sulfide scale. [3]

OSHA lists organic acids, with hydrogen sulfide, among the corrosive agents in the atmospheric tower, vacuum furnace and vacuum tower of crude units [1]. High-shear spots such as elbows and thermowells are frequent locations [3].

## How is it found and monitored?

- **Wall thickness measurement.** Ultrasonic testing measures general metal loss [6].
- **Corrosion coupons.** Field tests have used steel coupons and coupon racks exposed in furnaces and lines [3].
- **Acid number of the feed.** Titration of crude and fractions tracks how acidic the oil is [3].
- **Electrochemical probes have limits.** Linear polarization measurements are hampered by uncertain potential readings in hot oil [3].

Measures named in the 1986 review include removing acids by predistillation, blending crudes, neutralization, material selection and, above all, flow control [2]. OSHA notes that caustic treating removes naphthenic acids from product streams [1]. API RP 571 lists NAC among refinery damage mechanisms [3]; API's catalog shows its current edition as the 3rd (March 2020) [5].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Atmospheric and vacuum furnace tubes and transfer lines | High velocity and vaporization of acidic oil [3] | Wall thickness measurement; coupon racks in field tests [3][6] | [What is a fired heater?](/library/fired-heater/) |
| Vacuum column gas oil sections and packing | Acids condensing near their boiling range; some packed sections need 316 stainless steel even with low-acid feed [3] | Acid number of the gas oil streams [3] | [What is a crude distillation unit?](/library/crude-distillation-unit/) |
| Side-cut piping | Acid content; partial protection from sulfide scale [3] | Ultrasonic wall thickness measurement [6] | [How does ultrasonic thickness measurement work?](/library/ultrasonic-thickness-measurement/) |
| Elbows, thermowells and other high-shear spots | Wall shear stress, two-phase flow [3] | Ultrasonic thickness readings at those spots [6] | [Corrosion vs erosion vs erosion-corrosion: what is the difference?](/library/corrosion-vs-erosion/) |
| Units switching to more acidic crude | Changing crude blends and acid levels [3][4] | Crude acid number by ASTM D664 or D974 titration [3] | How do crude slate changes affect corrosion? |

Sources: Eun, Corrosion Science and Technology, 2008 [3]; Jin and others, 2018 [4]; OSHA Technical Manual, Section IV, Chapter 3 [6].

## Sources

1. [OSHA Technical Manual, Section IV, Chapter 2: Petroleum Refining Processes, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-2)
2. [Naphthenic Acid Corrosion in Petroleum Refineries. A Review (A. Jayaraman, H. Singh, Y. Lefebvre), Revue de l'Institut Francais du Petrole 41(2):265-274 (article page and abstract), Oil & Gas Science and Technology, IFP Energies nouvelles (open access)](https://ogst.ifpenergiesnouvelles.fr/10.2516/ogst:1986016)
3. [Corrosion and Materials Selection for Bitumen with Heavy Naphthenic Acid in Canadian Oil Sands (T. J.-C. Eun), Corrosion Science and Technology 7(6):350-361, Corrosion Science and Technology journal (Korea), via KoreaScience](https://koreascience.or.kr/article/JAKO200821161845188.pdf)
4. [High-Temperature Corrosion by Carboxylic Acids and Sulfidation under Refinery Conditions: Mechanism, Model, and Simulation (P. Jin, W. Robbins, G. Bota), Industrial & Engineering Chemistry Research 57:4329-4339, American Chemical Society; author copy hosted by Ohio University, Institute for Corrosion and Multiphase Technology](https://www.icmt.ohio.edu/documents/Journals2018/High%20Temperature%20Corrosion%20by%20Carboxylic%20Acids%20and%20Sulfidation%20under%20Refinery%20Conditions%20Mechanism,%20Model,%20and%20Simulation.pdf), 2018-03-07
5. [2025 Publications Catalog (entries for RP 571 and RP 939-C) (RP 571, 3rd edition, March 2020; RP 939-C, 2nd edition, January 2019), American Petroleum Institute (API)](https://www.api.org/-/media/files/publications/2025-catalog/2025_pubs%20catalog.pdf)
6. [OSHA Technical Manual, Section IV, Chapter 3: Pressure Vessel Guidelines, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-3)

Published by Winda Beacon (https://beacon.winda.ai).