# What is oxygen corrosion in water systems?

> Oxygen corrosion is metal loss caused by oxygen dissolved in water that is in contact with steel. Oxygen takes up the electrons that iron releases as it corrodes, so the amount of dissolved oxygen strongly affects the rate. Boiler feedwater, seawater injection and open cooling water systems limit it with deaeration, oxygen scavengers and inhibitors.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T15:24:40+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: Refining, Upstream and offshore
- Canonical: https://beacon.winda.ai/library/oxygen-corrosion/

## Why does it matter?

NASA's corrosion technology laboratory states that well over 90% of all corrosion reactions involve the reduction of oxygen [1]. In water systems the effect of oxygen can be measured in orders of magnitude. A 2019 Aalborg University paper on North Sea water injection puts dissolved oxygen in air-saturated seawater at about 5 to 8 mg/L and, citing earlier work, gives steel corrosion rates of 0.25 to 15 mm per year at those levels, falling to about 0.01 mm per year below 10 µg/L [2]. Offshore operators therefore strip oxygen out with vacuum deaerators and chemical scavengers before the water is injected [2].

## How does dissolved oxygen corrode steel?

Corrosion in water is electrochemical. Iron gives up electrons and goes into solution, and those electrons must be consumed by a reduction reaction somewhere else on the metal surface [1]. Reduction of dissolved oxygen is the most common such reaction, so the amount of oxygen present, and how easily it accepts electrons, is an important factor in how much metal is lost [1].

Because the oxygen reaction has a high reversible potential, its rate is typically limited by how fast oxygen diffuses to the steel rather than by the reaction step itself [4]. Flow therefore matters. In inhibited carbon dioxide (CO2) brine, in work cited by Ohio University researchers, film-forming inhibitors cut corrosion by about two orders of magnitude with less than 1 part per billion (ppb) of oxygen and flow made little difference; at 100 ppb, the rate depended on mass transfer [4].

Temperature matters too: the US Department of Energy (DOE) describes oxygen in a boiler system as a significant problem because of its corrosivity at high temperature [5]. Oxygen that gets into a system can be consumed close to where it entered, or it can accumulate in low-flow areas and cause localized corrosion [4].

## Where does oxygen get into oil, gas and utility water systems?

- **Production systems.** Hydrocarbon reservoirs normally contain no oxygen, yet contamination is common. It enters through leaks, maintenance work, equipment failures, chemical injection and poor procedures, at levels from ppb to parts per million (ppm) [4].
- **Seawater injection.** Injection water is pumped from near the sea surface, where dissolved oxygen is high [2]. Volumes are large: in the Danish North Sea, water injected in 2014 was 3.5 times the volume of oil produced [2].
- **Boiler feedwater and steam systems.** OSHA identifies dissolved gases, especially CO2 and oxygen, as a cause of boiler corrosion that deaeration and treatment remove [3]. DOE adds that air left in a steam system promotes condensate corrosion; air vents remove it [5].
- **Open cooling water.** Water cooled by contact with air in a cooling tower is saturated with oxygen, which OSHA notes increases the chance of corrosion [3].

## How is oxygen corrosion controlled and found?

**Deaeration.** A deaerator heats feedwater to saturation and breaks it into fine droplets or thin sheets so oxygen and other gases escape [5]. Pressurized deaerators and deaerating heaters reach about 7 to 40 ppb oxygen depending on design, while atmospheric deaerators typically leave 0.5 to 1 ppm [5]. OSHA describes deaerators as widely used in refining, chemicals, power and pulp and paper [6].

**Oxygen scavengers.** Where lower levels are needed, a chemical scavenger removes more oxygen and is usually part of the water treatment program [5]. In seawater injection, sulfite-based scavengers are common, but the sulfate they leave can feed sulfate-reducing bacteria that make hydrogen sulfide and sour corrosion, so dosing is a balance [2].

**Inhibitors.** In open cooling water, a substance that forms a protective film on metal surfaces is one way to prevent corrosion [3].

**Detection.** Dissolved oxygen instruments placed after the deaerator and scavenger injection can measure oxygen in real time; the 2019 study tested three commercial instruments for this role [2]. Electrochemical methods such as linear polarization resistance were used in the 2025 study to measure oxygen's effect on corrosion [4]. Where US gas pipelines carry corrosive gas, coupons or other monitoring devices must be checked twice each calendar year [7].

The deaerator itself needs inspection. OSHA reports that cracking in deaerator vessels was mostly corrosion fatigue at welds that had not been post-weld heat treated and that water hammer was the one operating factor linked to it; the industry recommendations it summarizes direct attention to internal welds and heat-affected zones, using wet fluorescent magnetic particle testing [6].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Boiler feedwater, economizer and boiler tubes | Dissolved oxygen and CO2 at high temperature [3][5] | Feedwater oxygen against deaerator capability: about 7 to 40 ppb pressurized, 0.5 to 1 ppm atmospheric [5] | [What is a fired heater?](/library/fired-heater/) |
| Deaerator and feedwater storage vessels | Water hammer; welds without post-weld heat treatment [6] | Wet fluorescent magnetic particle testing of internal welds and heat-affected zones [6] | What is corrosion fatigue?, [What are the main non-destructive testing (NDT) methods in oil and gas?](/library/ndt-methods-overview/) |
| Seawater injection systems | Air-saturated seawater at about 5 to 8 mg/L; scavenger under- or overdosing [2] | Dissolved oxygen instruments after the deaerator and scavenger injection [2] | [What is microbiologically influenced corrosion (MIC)?](/library/microbiologically-influenced-corrosion/) |
| Open recirculating cooling water | Water saturated with oxygen in the tower [3] | Water chemistry checks, including corrosion inhibitor levels [8] | [What is cooling water corrosion?](/library/cooling-water-corrosion/) |
| Production lines with oxygen ingress | Leaks, maintenance, chemical injection; low-flow areas [4] | Electrochemical monitoring such as linear polarization resistance [4]; coupons in corrosive gas pipelines [7] | [What is linear polarization resistance (LPR) monitoring?](/library/linear-polarization-resistance/), [Corrosion coupons vs electrical resistance (ER) probes](/library/corrosion-coupons-vs-er-probes/) |

Sources: Durdevic and Yang, 2019 [2]; OSHA Technical Manual, Section IV, Chapters 2 and 3 [3][6]; Deshmukh et al., 2025 [4]; DOE steam sourcebook, 2012 [5]; 49 CFR 192.477 [7]; EPA WaterSense at Work, 2012 [8].

## Sources

1. [Corrosion Fundamentals, NASA Kennedy Space Center, Corrosion Technology Laboratory](https://public.ksc.nasa.gov/corrosion/corrosion-fundamentals/)
2. [Potential use of real-time dissolved oxygen sensors for oxygen scavenging feedback control (P. Durdevic, Z. Yang), IOP Conference Series: Materials Science and Engineering 504, 012098, Aalborg University; IOP Publishing (CC BY 3.0)](https://vbn.aau.dk/ws/files/319152282/Durdevic_2019_IOP_Conf._Ser._Mater._Sci._Eng._504_012098.pdf)
3. [OSHA Technical Manual, Section IV, Chapter 2: Petroleum Refining Processes, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-2)
4. [Effects of Oxygen on Corrosion Inhibition in Sweet Systems (S. Deshmukh, Y. He, X. Wang, D. Young, M. Singer), AMPP Annual Conference paper C2025-00530, Ohio University, Institute for Corrosion and Multiphase Technology (author copy)](https://www.icmt.ohio.edu/documents/AMPP2025/c2025-00530%20SD%20Yi%20He.pdf)
5. [Improving Steam System Performance: A Sourcebook for Industry, Second Edition (DOE/GO-102012-3423), US Department of Energy, Advanced Manufacturing Office](https://www.energy.gov/sites/prod/files/2014/05/f15/steamsourcebook.pdf)
6. [OSHA Technical Manual, Section IV, Chapter 3: Pressure Vessel Guidelines, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-3)
7. [49 CFR 192.477, Internal corrosion control: Monitoring, US Government Publishing Office, Electronic Code of Federal Regulations (eCFR)](https://www.ecfr.gov/current/title-49/subtitle-B/chapter-I/subchapter-D/part-192/subpart-I/section-192.477)
8. [WaterSense at Work: Best Management Practices for Commercial and Institutional Facilities, Section 6.3 Cooling Towers, US Environmental Protection Agency (EPA)](https://www.epa.gov/system/files/documents/2023-05/ws-commercial-watersense-at-work_Section_6.3_Cooling_Towers.pdf)

Published by Winda Beacon (https://beacon.winda.ai).