# Radiographic vs ultrasonic testing for welds

> Radiographic testing (RT) images a weld with X-rays or gamma rays, while ultrasonic testing (UT) sends sound into it and reads the echoes. RT is better at volumetric flaws such as porosity and slag; UT is better at planar flaws such as cracks and lack of fusion, and can measure their through-wall height.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T09:44:04+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: LNG, Pipelines, Refining, Upstream and offshore
- Canonical: https://beacon.winda.ai/library/radiography-vs-ultrasonic/

## Why does it matter?

A radiograph can show no crack in a weld that has one. The Federal Aviation Administration (FAA) inspection guidance states that radiography detects cracks only when they lie close to the direction of the beam, and that tight cracks in thick sections may not show even when properly aligned [1]. UK Health and Safety Executive (HSE) guidance adds that crack detection depends on how open the crack is and how far the beam is from its plane, and that in many cases cracks will not be found [2]. The method chosen therefore limits which flaws a clean weld record can rule out [1][2].

## Radiographic vs ultrasonic testing at a glance

| | Radiographic testing (RT) | Ultrasonic testing (UT) |
|---|---|---|
| How it works | Radiation passes through the weld; flaws change how much reaches the film or detector [1][3] | Sound pulses enter the weld; flaws and surfaces send echoes back [2][3] |
| Best at | Volumetric flaws: porosity, slag, inclusions [1][2] | Planar flaws: cracks, lack of fusion [1][2] |
| Weak at | Tight or misaligned cracks [1][2]; laminations are nearly impossible to see [1] | Flaws not facing the beam [1]; coarse-grained austenitic and nickel alloy welds without special techniques [2] |
| Depth and height of a flaw | Not shown without special techniques [1][3] | Length and through-wall height can be measured [2] |
| Sensitivity measure | Image quality indicator of wires, holes or steps; about a 2% difference in absorption is detectable [1][2] | Echo height against a reference reflector, such as a 1.5 mm side-drilled hole in the US bridge welding code [4] |
| Record | Film or digital image kept as a permanent record [1][3] | None in basic manual form; automated and phased array systems store data [3][5] |
| Field thickness | Portable X-ray tubes limited to about 75 mm (3 in) of steel; higher-energy sources for thicker sections [1] | A wide range of materials and thicknesses [1] |
| Safety | Ionizing radiation: controlled areas, shielding and licensing [2][7][8] | No radiation; a couplant is usually needed [1] |
| Skill | High skill for exposure and interpretation [1] | High skill to set up and interpret [1] |

Sources: FAA AC 43.13-1B, Chapter 5 [1]; HSE COMAH technical measures document [2]; OSHA Technical Manual, Section IV, Chapter 3 [3]; FHWA-HRT-04-124 and 14-074 [4][5]; OSHA ionizing radiation pages [7]; 10 CFR 34.41 [8].

The FAA sums up the trade-off: both methods can find flaws deep inside a part, but radiography works better when flaws are not planar and ultrasonics works better when they are [1].

## When is radiographic testing used?

- **New welds where volumetric flaws matter and a film record is wanted.** RT shows porosity and slag well and leaves an image that can be reviewed later [1][2].
- **Where a code calls for it.** In 2014 the US bridge welding code required RT for complete joint penetration welds under tension and did not yet recognize phased array UT [5].
- **Corrosion under insulation on small pipe.** Flash radiography with the beam tangential to the pipe shows external corrosion as changes in the wall profile, normally on pipe up to 12 in (about 300 mm) outside diameter [2].
- **Covered or hidden parts,** which the FAA lists among radiography's advantages [1].

## When is ultrasonic testing used?

- **Finding and sizing planar flaws,** such as fatigue cracks or lack of sidewall fusion, because UT gives the through-wall height that an engineering critical assessment of a flaw relies on [2].
- **Thick sections,** where portable radiography is slow or limited by source output [1].
- **Work beside running plant.** RT needs a controlled area around the source; HSE describes radiography systems designed to shrink it to about 3 m so nearby work is less affected [2]. UT needs no such area.
- **Mechanized and phased array scans.** In FHWA bridge weld tests, phased array UT located the same flaws as radiographs and also gave their depth, which radiographs could not [6].

## What do people often get wrong?

Two assumptions cause most confusion. The first is that a sharp image means a sensitive test: HSE notes that the image quality indicator shows only the ability to see changes in section or wire size, which relates only indirectly to finding real flaws [2]. The second is that UT echo height equals flaw size: FHWA notes that amplitude also depends on flaw type, orientation, roughness and reflectivity [4].

Acceptance rules reflect the physics. HSE gives the example of the UK pressure vessel specification PD 5500, in which radiography allows no cracks, while ultrasonic acceptance limits planar indications by height, length and amplitude [2].

## Where integrity problems show up

| What it finds well | What it can miss or get wrong | In the Library |
|---|---|---|
| Porosity, slag and inclusions in new welds, with RT [1][2] | Tight cracks, cracks off the beam axis and laminations [1][2] | [How is fabrication quality controlled for pressure equipment?](/library/fabrication-quality-control/) |
| Flaw position along the weld on a radiograph [6] | The depth of the flaw in the wall [3][6] | How are crack-like flaws assessed for fitness-for-service? |
| Wall profile of small insulated pipe, with tangential RT [2] | Fine detail: contrast and resolution are lower than in normal radiography [2] | [What is corrosion under insulation (CUI)?](/library/corrosion-under-insulation/) |
| Weld flaws in site-built LPG vessels, where manual UT gave the best trial results [2] | Fabrication hydrogen cracking, which HSE calls very difficult to detect with radiography [2] | [What is hydrogen embrittlement?](/library/hydrogen-embrittlement/) |
| Planar flaws and their height, with UT [2] | Skewed flaws and operator differences; in one study, vertical cracks up to 40% of plate thickness could be accepted in nearly a third of manual inspections [4] | [Ultrasonic testing](/glossary/ultrasonic-testing/) |

Sources: FAA AC 43.13-1B [1]; HSE COMAH technical measures document, including its LPG vessel case study [2]; OSHA Technical Manual [3]; FHWA-HRT-04-124 and 14-075 [4][6].

## Sources

1. [Advisory Circular AC 43.13-1B, Acceptable Methods, Techniques, and Practices: Aircraft Inspection and Repair, Chapter 5: Nondestructive Inspection (NDI), US Federal Aviation Administration (FAA)](https://www.faa.gov/documentLibrary/media/Advisory_Circular/AC_43.13-1B_w-chg1.pdf)
2. [Inspection/Non Destructive Testing (COMAH technical measures document), UK Health and Safety Executive (HSE)](https://www.hse.gov.uk/comah/sragtech/techmeasndt.htm)
3. [OSHA Technical Manual, Section IV, Chapter 3: Pressure Vessel Guidelines, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-3)
4. [Lab and Field Testing of AUT Systems for Steel Highway Bridges (FHWA-HRT-04-124), Chapter 2: Background, US Federal Highway Administration (FHWA)](https://www.fhwa.dot.gov/publications/research/infrastructure/structures/04124/02.cfm)
5. [Development of Phased-Array Ultrasonic Testing Acceptability Criteria (Phase I), TechBrief FHWA-HRT-14-074, US Federal Highway Administration (FHWA)](https://www.fhwa.dot.gov/publications/research/infrastructure/structures/bridge/14074/index.cfm)
6. [Development of Phased-Array Ultrasonic Testing Acceptability Criteria (Phase II), TechBrief FHWA-HRT-14-075, US Federal Highway Administration (FHWA)](https://www.fhwa.dot.gov/publications/research/infrastructure/structures/bridge/14075/index.cfm)
7. [Ionizing Radiation: Hazards, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/ionizing-radiation/hazards)
8. [10 CFR 34.41, Conducting industrial radiographic operations, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-10/section-34.41)
9. [49 CFR 192.243, Nondestructive testing, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/section-192.243)
10. [Ionizing Radiation: Control and Prevention, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/ionizing-radiation/control-prevention)

Published by Winda Beacon (https://beacon.winda.ai).