# What is stress corrosion cracking (SCC)?

> Stress corrosion cracking (SCC) is cracking caused by tensile stress and a corrosive environment acting together on a susceptible metal. All three must be present; take any one away and SCC does not occur. The cracks can run deep while the surrounding surface shows little corrosion, so thickness readings alone do not reveal them.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T09:44:04+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: LNG, Pipelines, Refining
- Canonical: https://beacon.winda.ai/library/stress-corrosion-cracking/

## Why does it matter?

Stress corrosion cracks can grow through a wall while the metal around them shows little or no corrosion, and the crack surfaces themselves are barely corroded [1]. The US National Institute of Standards and Technology (NIST) notes that such crack-like flaws harm structural integrity far more than the small amount of metal involved, and that they tend to form where stress is highest [1]. Surveys summarized by NIST in 1990 and by OSHA found cracking in about half of the ammonia storage vessels examined and in about 40% of 294 amine plants [1][2].

## What conditions cause SCC?

NIST lists three conditions that must act together: a susceptible material or material condition, a chemically aggressive environment, and high enough tensile stress [1]. A 2005 study for US pipeline regulators sets out the same three [3].

- **Stress.** It can be applied in service or left behind by welding, forming, machining or grinding; welding residual stress can approach the yield strength [1][4]. Below a threshold stress, cracks may not start, but NIST notes that little such data exists for carbon steels in plant environments [1].
- **Material condition.** Susceptibility generally rises with hardness and strength, so high-strength bolts and weld heat-affected zones that were not stress relieved are typical weak spots [1].
- **Environment and temperature.** Each alloy cracks only in particular environments, and cracking generally gets worse as temperature rises [4].

## Which metals and environments are involved?

| Metal | Environments linked to SCC | In the Library |
|---|---|---|
| Carbon and low-alloy steel | Hot caustic, nitrates, wet hydrogen sulfide (H2S), anhydrous ammonia, amine solutions, hot oxygenated water [1]; carbonate and bicarbonate solutions [4] | Caustic stress corrosion cracking |
| Buried pipeline steel | Concentrated carbonate-bicarbonate (high pH) or dilute groundwater with dissolved carbon dioxide (near-neutral pH), under disbonded coating [3] | [Pipeline SCC](/library/pipeline-stress-corrosion-cracking/) |
| Austenitic stainless steel | Hot chloride solutions, chloride with H2S, caustic [4] | Chloride stress corrosion cracking |
| Copper alloys | Ammonia and amines [4] | What are the main types of corrosion? |

## What does SCC look like?

Cracks usually run across the main stress direction, either as one crack or as a branching network, and may follow the grain boundaries (intergranular) or cut through the grains (transgranular) [1]. On buried pipelines, SCC shows up as groups of many small, parallel cracks close together on the pipe's outer surface, which can link up and cause a leak or rupture [3]. High-pH pipeline SCC is mainly intergranular with tight cracks; near-neutral pH SCC is mainly transgranular with wider, corroded crack walls [3].

## How is SCC found?

- **Wet fluorescent magnetic particle testing (WFMT)** was the preferred internal method in the amine survey and, with proper surface preparation, the most effective method on caustic digesters [2].
- **Magnetic particle testing** works only on ferromagnetic carbon and low-alloy steels; **liquid penetrant testing** also works on austenitic stainless steels and nonferrous alloys [2].
- **Radiography** has trouble with tight, closed cracks; **ultrasonic testing** finds flaws inside the wall [2].
- **Pipelines:** hydrostatic testing, in-line inspection (ultrasonic, electromagnetic acoustic transducer and transverse field tools), direct examination at excavations, and direct assessment [3].

OSHA's guidance points out that safety assessment depends on "the largest flaw that may be missed, not the smallest one that can be found" [2].

## How is SCC controlled?

Because SCC needs all three conditions, control measures target one of them [1]. Measures described in public sources include choosing a more resistant alloy, lowering stress through stress relief or post-weld heat treatment (PWHT), removing harmful species such as oxygen, coatings, cathodic protection for some chloride cases (which can bring a risk of hydrogen embrittlement) and inhibitors [4]. On pipelines, the PHMSA study states that SCC does not occur beneath an intact coating that keeps groundwater off the steel [3]. For amine units, API publishes RP 945, *Avoiding Environmental Cracking in Amine Units* (4th edition, September 2022) [5].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Amine absorbers, regenerators, exchangers and piping | Amine with carbon dioxide; welds without PWHT; most common in monoethanolamine units [2] | Internal WFMT, the preferred method, and ultrasonic testing [2] | What is amine corrosion and amine cracking? |
| Ammonia storage spheres | Water and oxygen content of the ammonia; as-welded vessels [1][2] | Weld inspection; cracks run both along and across welds [2] | What are the main non-destructive testing (NDT) methods in oil and gas? |
| Vessels in hot caustic service (survey data from pulp digesters) | Caustic at welds that were not fully stress relieved [2] | WFMT with proper surface preparation [2] | What is caustic stress corrosion cracking? |
| Austenitic stainless steel equipment | Hot chloride solutions with residual stress [4] | Liquid penetrant testing [2] | What is chloride stress corrosion cracking? |
| Buried transmission pipelines | Disbonded coating with high-pH or near-neutral pH groundwater [3] | In-line inspection, hydrostatic testing, direct assessment [3] | [What is stress corrosion cracking in pipelines (high-pH and near-neutral pH)?](/library/pipeline-stress-corrosion-cracking/) |
| Vessels and welds in wet H2S service | Hard weld zones in water containing H2S [1][2] | WFMT and ultrasonic testing [1][2] | What is wet hydrogen sulfide (H2S) damage? |

Sources: NIST SP 780, 1990 [1]; OSHA Technical Manual, Section IV, Chapter 3 [2]; PHMSA SCC study, 2005 [3]; KFUPM course notes [4].

## Sources

1. [NIST Special Publication 780, Guidelines for Pressure Vessel Safety Assessment (S. Yukawa), US National Institute of Standards and Technology (NIST)](https://nvlpubs.nist.gov/nistpubs/Legacy/SP/nistspecialpublication780.pdf)
2. [OSHA Technical Manual, Section IV, Chapter 3: Pressure Vessel Guidelines, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-3)
3. [Stress Corrosion Cracking Study (TTO Number 8, Integrity Management Program), prepared by Michael Baker Jr., Inc. for the Office of Pipeline Safety, US Pipeline and Hazardous Materials Safety Administration (PHMSA), then Research and Special Programs Administration](https://www.phmsa.dot.gov/sites/phmsa.dot.gov/files/docs/technical-resources/pipeline/hazardous-liquid-integrity-management/62751/sccreport-finalreportwithoutdatabase.pdf)
4. [Corrosion Engineering course notes, 4.6 Stress Corrosion Cracking (pages 1 to 4), King Fahd University of Petroleum and Minerals (KFUPM), Mechanical Engineering faculty pages](https://faculty.kfupm.edu.sa/ME/hussaini/Corrosion%20Engineering/04.06.01.htm)
5. [2025 Publications Catalog (entries for RP 571 and RP 945) (RP 571, 3rd edition, March 2020; RP 945, 4th edition, September 2022), American Petroleum Institute (API)](https://www.api.org/-/media/files/publications/2025-catalog/2025_pubs%20catalog.pdf)