# What is temper embrittlement?

> Temper embrittlement is a loss of toughness in low-alloy steels, such as 2.25Cr-1Mo, after long exposure to, or slow cooling through, a range of roughly 320 to 525 °C. Impurities such as phosphorus, tin and antimony gather at grain boundaries. The steel keeps its strength but can break in a brittle way when it is cool.

- Label: Fact
- Type: Explainer
- Published: 2026-11-13T15:24:40+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-13
- Topics: Refining
- Canonical: https://beacon.winda.ai/library/temper-embrittlement/

## Why does it matter?

The loss therefore shows up when equipment is cool, not at operating temperature. For heavy wall chromium-molybdenum reactors in high-pressure hydrogen service, the American Petroleum Institute (API) has published technical reports since 2017 on setting a minimum pressurization temperature for start-ups and shutdowns of temper-embrittled 2.25Cr-1Mo steel in high-pressure hydrogen [4]. Brittle fracture needs a crack-like flaw, high stress and low toughness together, so lost toughness makes any flaw more serious [5].

## What happens inside the steel?

During long exposure in the embrittling range, impurity atoms move to the boundaries of the former austenite grains and weaken the bond between neighboring grains [1]. The main embrittling elements are antimony, phosphorus, tin and arsenic; a 1977 review found antimony and tin the most effective, and noted that alloying elements encourage the impurities to segregate [1]. In chromium-molybdenum steels without nickel, a 1980 technical report found phosphorus the main culprit, with manganese and silicon making it worse through their interaction with phosphorus [2]. Grain boundary chemistry, grain size and hardness together set how far the transition temperature moves [2].

Sources give the damaging range differently: the 1977 review gives 320 to 525 °C [1], and a study published by API exposed chromium-molybdenum steels at 650 to 950 °F (343 to 510 °C) [3].

The damage can be undone: the 1977 review treats temper embrittlement as reversible [1], and the API-published study included repeated de-embrittlement of two embrittled steels [3].

## Which equipment is at risk?

- **Heavy wall hydroprocessing reactors.** API Publication 959 (1st edition, January 1982) characterized 64 commercial chromium-molybdenum steel samples, mostly 2.25Cr-1Mo, heat treated as for hydrotreater reactor fabrication; API notes that steel made up to about 1975 does not represent the low-susceptibility plate, forgings and weld metal generally available after 1975 [4][3]. API RP 934-A (3rd edition, January 2019) covers materials and fabrication of new heavy wall 2.25Cr and 3Cr steel vessels that will operate in hydrogen at high temperature and pressure [4]. See [What is hydroprocessing (hydrotreating and hydrocracking)?](/library/hydroprocessing/).
- **Steam turbine rotors.** Chromium-molybdenum-vanadium rotors sampled after 15 to 26 years of service showed in-service temper embrittlement; phosphorus was the only residual element with a significant effect, and coarse grains raised susceptibility [6].

## How is it tested and found?

- **Step cooling.** A step-cooling heat treatment reveals susceptibility in the laboratory, and a 1989 study found it can simulate long-term service embrittlement except in very coarse-grained steel [6].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Heavy wall 2.25Cr-1Mo hydroprocessing reactors | Years in the embrittling range; impurity content of plate, forgings and weld metal [3][4] | Charpy tests on step-cooled or exposed samples [3] | [What is hydroprocessing (hydrotreating and hydrocracking)?](/library/hydroprocessing/) |
| Reactors at start-up and shutdown | Pressure applied while the embrittled steel is cool and holds dissolved hydrogen [4] | Not found by inspection; managed with minimum pressurization temperature limits, the subject of API's TR 934-F reports [4] | [Minimum design metal temperature (MDMT)](/glossary/minimum-design-metal-temperature/) |
| Embrittled vessels with crack-like flaws | Flaw, high stress and low toughness together [5] | Inspection for crack-like flaws; NIST notes flaws can sit in uninspected areas or be missed [5] | [What are the main non-destructive testing (NDT) methods in oil and gas?](/library/ndt-methods-overview/) |
| Steam turbine rotors (CrMoV) | 15 to 26 years in service; coarse grains [6] | Transition temperature shift measured on samples [6] | What is brittle fracture? |

Sources: Shaw, 1981 [3]; API 2025 catalog [4]; NIST SP 780, 1990 [5]; Cheruvu and Seth, 1989 [6].

## Sources

1. [Reversible temper embrittlement (D. F. Stein), Annual Review of Materials Science 7 (record and abstract), US DOE Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/6490342)
2. [Elimination of impurity-induced embrittlement in steel. Part 1: impurity segregation and temper embrittlement (C. J. McMahon Jr. and others), technical report (record and abstract), US DOE Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/5078844)
3. [Characterization study of temper embrittlement of chromium-molybdenum steels (B. J. Shaw), Proceedings, API Refining Department, vol. 60 (record and abstract), US DOE Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/6436478)
4. [2025 Publications Catalog (entries for Publ 959, RP 934-A and TR 934-F, Part 1) (Publ 959, 1st edition, January 1982; RP 934-A, 3rd edition, January 2019; TR 934-F, Part 1, 1st edition, 2017), American Petroleum Institute (API)](https://www.api.org/-/media/files/publications/2025-catalog/2025_pubs%20catalog.pdf)
5. [NIST Special Publication 780, Guidelines for Pressure Vessel Safety Assessment (S. Yukawa), US National Institute of Standards and Technology (NIST)](https://nvlpubs.nist.gov/nistpubs/Legacy/SP/nistspecialpublication780.pdf)
6. [The influences of impurity content, tensile strength, and grain size on in-service temper embrittlement of CrMoV steels (N. S. Cheruvu, B. B. Seth), Metallurgical Transactions A 20A (record and abstract), US DOE Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/6816154)

Published by Winda Beacon (https://beacon.winda.ai).