# What are the main types of corrosion?

> Corrosion types are grouped by how the damage looks and what drives it: general thinning, localized attack, galvanic, cracking and high-temperature forms. US Army Corps of Engineers specifications list eight classic forms, while API RP 571 (3rd edition, 2020) covers over 60 damage mechanisms in refining. Localized forms can perforate a wall with little total metal loss.

- Label: Fact
- Type: Explainer
- Published: 2026-11-14T12:02:06+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-14
- Topics: Pipelines, Refining, Upstream and offshore
- Canonical: https://beacon.winda.ai/library/types-of-corrosion/

## Why does it matter?

In 2019 the UK Health and Safety Executive (HSE) described an 8-inch refinery relief line that was thickness-tested at four fixed points, yet ruptured from highly localized internal corrosion elsewhere and released about 75 tonnes of flammable material [5]. Readings at fixed points missed it because the attack was local [5]. Pitting can cause failure by perforation with only a small loss of total weight, and pits are often small and hidden under corrosion products [2].

## How many types of corrosion are there?

It depends on who is counting and on what basis: the three schemes in the table range from 8 forms to more than 60 mechanisms [2][1][4]. After the table, the Library sorts mechanisms into four families, each with one line and a link. For what corrosion is and why metal corrodes, see [What is corrosion?](/library/corrosion/).

| Scheme | Count | Basis |
|---|---|---|
| Classic forms, as listed in US military guide specifications | 8 | Appearance of the corroded metal [2] |
| NASA Kennedy Space Center corrosion laboratory | 16 | Appearance and cause, including fretting and corrosion in concrete [1] |
| API RP 571, 3rd edition (2020) | Over 60 | Damage mechanisms affecting fixed equipment in refining [4] |

## What are the forms of metal loss?

- **[Uniform and localized metal loss](/glossary/metal-loss/)**: general thinning is the most common form and is usually noticed early; local attack is harder to see [1][2].
- **[Pitting](/library/pitting-corrosion/)**: small, deep cavities that can perforate a wall with little overall loss [2].
- **[Crevice](/library/crevice-corrosion/)**: attack in tight gaps under gaskets, washers and threads where liquid stagnates [1][2].
- **[Under-deposit](/library/under-deposit-corrosion/)**: oxygen-starved areas under deposits become anodes and corrode [1].
- **[Galvanic](/library/galvanic-corrosion/)**: the more active of two connected metals corrodes in a shared electrolyte [1].
- **[Carbon dioxide (CO2)](/library/co2-corrosion/)**: dissolved CO2 acidifies water inside pipelines; see [sweet vs sour corrosion](/library/sweet-vs-sour-corrosion/) [8][9].
- **[Microbiologically influenced (MIC)](/library/microbiologically-influenced-corrosion/)**: microbes in biofilms and deposits create aggressive local chemistry [1][9].
- **[Under insulation (CUI)](/library/corrosion-under-insulation/)**: water trapped under lagging, one of the most common mechanisms HSE lists [20][1].
- **[Atmospheric](/library/atmospheric-corrosion/)**: attack by moisture in air, a common external type [8].
- **[Soil](/library/soil-corrosion/)**: external attack on buried metal from the surrounding ground [8].
- **[Oxygen in water systems](/library/oxygen-corrosion/)**: dissolved oxygen corrodes boiler systems unless removed by deaeration and treatment [6].
- **[Cooling water](/library/cooling-water-corrosion/)**: air-cooled, oxygen-saturated recirculating water raises corrosion risk [6].
- **[Hydrochloric acid (HCl)](/library/hydrochloric-acid-corrosion/)**: crude salts release hydrogen chloride that condenses as acid in overheads [6].
- **[Ammonium chloride](/library/ammonium-chloride-corrosion/)**: salt deposits corrode once wetted, without enough wash water [6].
- **[Top-of-line](/library/top-of-line-corrosion/)**: corrosive vapor condenses on the cooler top of wet gas lines [15].
- **[Flue gas dew point](/library/flue-gas-dew-point-corrosion/)**: flue gas cooled below its dew point condenses and can corrode stacks and stack liners [17][6].

## What are the forms of environmental cracking?

- **[Stress corrosion cracking (SCC)](/library/stress-corrosion-cracking/)**: needs a susceptible material, a specific environment and tensile stress together [3].
- **[Wet hydrogen sulfide (H2S) damage](/library/wet-h2s-damage/)**: absorbed hydrogen blisters and cracks steel, especially at hard weld zones [7][3]. Forms: [blistering](/glossary/hydrogen-blistering/), [hydrogen induced cracking (HIC)](/glossary/hydrogen-induced-cracking/), [stress oriented hydrogen induced cracking (SOHIC)](/glossary/stress-oriented-hydrogen-induced-cracking/), [sulfide stress cracking (SSC)](/glossary/sulfide-stress-cracking/); compared in [HIC vs SOHIC vs SSC](/library/hic-vs-sohic-vs-ssc/).
- **[Amine](/library/amine-corrosion/)**: cracking in or near welds, mostly those without post-weld heat treatment [7].
- **[Caustic SCC](/library/caustic-stress-corrosion-cracking/)**: hot caustic cracks carbon steel at welds [3][7].
- **[Chloride SCC](/library/chloride-stress-corrosion-cracking/)**: chlorides crack hot austenitic stainless steel, as under wet insulation [1].
- **[Polythionic acid SCC](/library/polythionic-acid-scc/)**: sulfide scale meets air and moisture at shutdown and cracks sensitized stainless [14].
- **[Intergranular](/library/intergranular-corrosion/)**: attack along grain boundaries, as in [sensitized](/glossary/sensitization/) stainless near welds [1][2].
- **[Hydrogen embrittlement](/library/hydrogen-embrittlement/)**: absorbed hydrogen makes high-strength steels crack [1][2].
- **[Corrosion fatigue](/library/corrosion-fatigue/)**: cyclic stress plus corrosion does more than either alone [1].
- **[Pipeline SCC](/library/pipeline-stress-corrosion-cracking/)**: crack colonies on buried pipe under disbonded coating [10][11].
- **[Carbonate SCC](/library/carbonate-stress-corrosion-cracking/)**: cracking in carbonate-bicarbonate environments, which US rules require operators to evaluate [11].

## What happens at high temperature?

- **[High temperature hydrogen attack (HTHA)](/library/high-temperature-hydrogen-attack/)**: hydrogen reacts with carbon in hot steel, forming methane and fissures [13].
- **[Sulfidation](/library/sulfidation/)**: hot sulfur compounds thin steel, fastest in low-silicon carbon steel [12].
- **[Naphthenic acid](/library/naphthenic-acid-corrosion/)**: crude acids attack above about 230 °C (450 °F) when the acid value is high [6].
- **[High-temperature oxidation](/library/high-temperature-oxidation/)**: metal wastes to oxide in hot, oxygen-bearing gas [3][16].
- **[Carburization](/library/carburization/)**: carbon diffuses into furnace tubes and embrittles them [18][16].
- **[Metal dusting](/library/metal-dusting/)**: a carbon-driven attack favored, like carburization, by coke on hot tubes [16].
- **[Creep](/library/creep/)**: slow, permanent stretching under stress at high temperature [19].
- **[Short-term overheating](/library/short-term-overheating/)**: tubes run too hot; HSE lists overheating among common failure causes [20][19].

## Which mechanical damage is managed alongside corrosion?

- **[Erosion and erosion-corrosion](/library/corrosion-vs-erosion/)**: wear by solids and flow, or flow stripping protective films [21].
- **[Cavitation](/library/cavitation/)**: collapsing vapor bubbles erode pump surfaces [20].
- **[Mechanical and vibration fatigue](/library/mechanical-vibration-fatigue/)**: cracking from repeated stress cycles [3].
- **[Thermal fatigue](/library/thermal-fatigue/)**: cracking from repeated temperature changes [3].
- **[Brittle fracture](/library/brittle-fracture/)**: sudden cracking from a flaw, high stress and low toughness [3].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Piping, vessels and pipelines (metal loss) | Water, oxygen, CO2, H2S, acids, chlorides, deposits, stagnant flow [6][8][9] | Ultrasonic thickness readings and in-line inspection; local loss can fall between fixed points [7][8][5] | [Ultrasonic thickness measurement](/library/ultrasonic-thickness-measurement/), [Condition monitoring locations](/library/condition-monitoring-locations/) |
| Welds in amine, wet H2S, caustic and ammonia service (cracking) | Susceptible steel, specific environment, residual stress [3][7] | Wet fluorescent magnetic particle and ultrasonic testing found most amine cracks [7] | [NDT methods](/library/ndt-methods-overview/) |
| Buried pipelines (cracking) | Disbonded coating, carbonate-bicarbonate environment [10][11] | Crack in-line inspection and SCC direct assessment [10][11] | [Direct assessment](/library/direct-assessment/), [In-line inspection](/library/in-line-inspection/) |
| Hot hydrogen and sulfur service (high temperature) | Temperature, hydrogen, sulfur, steel composition [12][13] | Every component in low-silicon-prone circuits; HTHA is hard to detect by inspection [12][13] | [Damage mechanism review](/library/damage-mechanism-review/), [Integrity operating windows](/library/integrity-operating-windows/) |

Sources: HSE safety alert, 2019 [5]; OSHA [6][7]; PHMSA [8]; NTSB [9][10]; 49 CFR 192.929 [11]; CSB [12][13].

## Sources

1. [Forms of Corrosion, NASA Kennedy Space Center, Corrosion Technology Laboratory](https://public.ksc.nasa.gov/corrosion/forms-of-corrosion/)
2. [UFGS 26 42 17, Impressed Current Cathodic Protection (ICCP) System (section 1.2, definitions of corrosion forms), US Army Corps of Engineers, NAVFAC and AFCEC (Unified Facilities Guide Specifications), via WBDG](https://legacy.wbdg.org/FFC/DOD/UFGS/UFGS%2026%2042%2017.pdf)
3. [NIST Special Publication 780, Guidelines for Pressure Vessel Safety Assessment (S. Yukawa), US National Institute of Standards and Technology (NIST)](https://nvlpubs.nist.gov/nistpubs/Legacy/SP/nistspecialpublication780.pdf)
4. [2025 Publications Catalog (entry for RP 571, Damage Mechanisms Affecting Fixed Equipment in the Refining Industry) (RP 571, 3rd edition, March 2020), American Petroleum Institute (API)](https://www.api.org/-/media/files/publications/2025-catalog/2025_pubs%20catalog.pdf)
5. [Catastrophic rupture of dead-leg pipe-work (Safety alert, Bulletin No. CEMHD2-2019), UK Health and Safety Executive (HSE)](https://www.hse.gov.uk/safetybulletins/catastrophic-rupture-dead-leg-pipe-work.htm), 2019-08-20
6. [OSHA Technical Manual, Section IV, Chapter 2: Petroleum Refining Process, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-2)
7. [OSHA Technical Manual, Section IV, Chapter 3: Pressure Vessel Guidelines, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-3)
8. [Fact Sheet: Corrosion, US Pipeline and Hazardous Materials Safety Administration (PHMSA)](https://primis.phmsa.dot.gov/stakeholder-comms/factsheets/fscorrosion/)
9. [Pipeline Accident Report NTSB/PAR-03/01: Natural Gas Pipeline Rupture and Fire Near Carlsbad, New Mexico, August 19, 2000, US National Transportation Safety Board (NTSB)](https://www.ntsb.gov/investigations/AccidentReports/Reports/PAR0301.pdf)
10. [Pipeline Accident Report NTSB/PAR-12/01: Enbridge Incorporated Hazardous Liquid Pipeline Rupture and Release, Marshall, Michigan, July 25, 2010, US National Transportation Safety Board (NTSB)](https://www.ntsb.gov/investigations/AccidentReports/Reports/PAR1201.pdf)
11. [49 CFR 192.929, What are the requirements for using Direct Assessment for Stress Corrosion Cracking?, eCFR, US Office of the Federal Register](https://www.ecfr.gov/current/title-49/subtitle-B/chapter-I/subchapter-D/part-192/subpart-O/section-192.929)
12. [Final Investigation Report: Chevron Richmond Refinery Pipe Rupture and Fire, US Chemical Safety and Hazard Investigation Board (CSB)](https://www.csb.gov/assets/1/17/Chevron_Final_Investigation_Report_2015-01-28.pdf?15397), 2015-01-28
13. [Investigation Report 2010-08-I-WA: Catastrophic Rupture of Heat Exchanger, Tesoro Anacortes Refinery, US Chemical Safety and Hazard Investigation Board (CSB)](https://www.csb.gov/assets/1/7/tesoro_anacortes_2014-may-01.pdf)
14. [Corrosion by Polythionic Acid in the Oil and Gas Sector: A Brief Overview (M. Vakili and others), Materials 16(21): 7043, MDPI (open access, CC BY 4.0)](https://doi.org/10.3390/ma16217043)
15. [The effect of mono ethylene glycol on the top of line corrosion rate of low carbon steel in acetic acid and elevated temperature environment (B. Widyanto and I. G. B. E. Suputra Wiguna), Heliyon 5(6): e02006, Elsevier (open access)](https://doi.org/10.1016/j.heliyon.2019.e02006)
16. [Investigation of the 0.4C-35Cr-45Ni-Nb Alloy after Service in High-Temperature Steam and Hydrocarbons Environment (J. Orlikowski and others), Materials 14(20): 6139, MDPI (open access, CC BY 4.0)](https://doi.org/10.3390/ma14206139)
17. [Energy Tips: Steam, Steam Tip Sheet #26A: Consider Installing a Condensing Economizer (DOE/GO-102012-3393), US Department of Energy, Advanced Manufacturing Office](https://www.energy.gov/sites/prod/files/2014/05/f16/steam26a_condensing.pdf)
18. [Impacts of Condition Assessment on Energy Use: Selected Applications in Chemicals Processing and Petroleum Refining (J. L. Pellegrino and T. M. Carole, Energetics Inc.), US Department of Energy, Industrial Technologies Program](https://www.energy.gov/sites/prod/files/2013/11/f4/condition_assessment.pdf)
19. [Creep Deformation of Metals (Teaching and Learning Package), DoITPoMS, University of Cambridge](https://www.doitpoms.ac.uk/tlplib/creep/index.php)
20. [Design Codes: Plant (COMAH technical measures), UK Health and Safety Executive (HSE)](https://www.hse.gov.uk/comah/sragtech/techmeasplant.htm)
21. [Guides to Good Practice in Corrosion Control No. 6: Corrosion Control for Pumps and Valves (R. Francis), National Physical Laboratory (NPL), UK](https://eprintspublications.npl.co.uk/8618/1/Corrosion%20Guide%20No%206.pdf)

Published by Winda Beacon (https://beacon.winda.ai).