# What is wet hydrogen sulfide (H2S) damage?

> Wet hydrogen sulfide (H2S) damage is hydrogen damage to carbon steel in water that contains H2S. Corrosion releases hydrogen into the steel, causing blistering, sulfide stress cracking (SSC), hydrogen-induced cracking (HIC) and its stress-oriented form (SOHIC). NACE MR0175/ISO 15156 sets material requirements for H2S service in oil and gas production.

- Label: Fact
- Type: Explainer
- Published: 2026-11-14T12:02:06+09:00
- By: Jun Zhong
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jun Zhong on 2026-11-14
- Topics: LNG, Refining, Upstream and offshore
- Canonical: https://beacon.winda.ai/library/wet-h2s-damage/

## Why does it matter?

On July 23, 1984, an amine absorber at a refinery in Romeoville, Illinois, ruptured; 17 people died, and OSHA reported damage of more than $100 million [4]. Investigators at the National Bureau of Standards (now NIST) found that cracks had started in hard metal formed during a repair weld, then grown through more than 90% of the wall by hydrogen pressure cracking [3]. Hydrogen had also cut the steel's fracture resistance by more than half, so the vessel broke at about 10% of the steel's rated strength, although measured wall thicknesses were within allowances [3].

## How does wet H2S damage steel?

When steel corrodes in water containing H2S, hydrogen is produced at the surface and part of it enters the metal as atoms [1]. Inside, the atoms collect at traps such as inclusions, voids and grain boundaries, recombine into hydrogen gas and build internal pressure [7]. Dissolved hydrogen can also lower ductility and fracture toughness without any visible flaw [2]. Sensitivity rises with the hardness and strength of the steel [1][2].

## What forms does wet H2S damage take?

| Form | What it looks like | What drives it |
|---|---|---|
| Hydrogen blistering | Surface bulges over internal voids parallel to the surface; a sign that hydrogen is entering [2] | Hydrogen gas collecting near the surface [2] |

Sources: NIST SP 780, 1990 [2]; Kazys and others, 2022 [7].

## Where does wet H2S damage occur?

- **Refinery pressure vessels.** A 1988 interim report from a refinery industry inspection program found cracks of varying severity in 31% of 189 vessels, more than expected, partly because a more sensitive examination method was used [2].
- **Liquefied petroleum gas (LPG) storage spheres.** A survey reported cracking in 30% of 141 vessels, part of it old fabrication flaws but part in-service cracking, mostly in weld heat-affected zones. The H2S was carried over from upstream treating, and incidence was higher in as-welded and higher-strength steels [2].
- **Crude, catalytic cracking and gas plants.** OSHA notes that wet H2S cracks steel in crude unit service, and that ammonia and cyanide from high-nitrogen feeds can cause corrosion, cracking or hydrogen blistering in catalytic cracking overhead systems [8].

## How is wet H2S damage found?

- **Wet fluorescent magnetic particle testing (WFMT)** of internal weld surfaces was the method used in the refinery inspection program and is more sensitive than older methods [2].
- **Visual examination** shows blistering on a clean, well-lit surface [1].
- **Ultrasonic testing** finds internal cracks. In a 1990s research program on welded plates in wet H2S, several ultrasonic methods used together sized HIC, SOHIC and SSC well, automated scans were more repeatable than manual ones, and no single method described the damage fully [5][6].
- **Newer ultrasonic imaging.** A 2022 study on refinery exchanger steel found total focusing method imaging resolved cracks close to 0.2 mm, and a low-angle time-of-flight diffraction probe suited screening large areas [7].
- **Hardness testing** has a known gap: significant cracks can start from very small hard zones at welds that conventional hardness tests do not detect [1].

## What limits it?

Measures described in US government guidance and industry sources include lower-strength steels for new vessels, weld hardness control, post-weld heat treatment (PWHT), which appears to reduce sensitivity to cracking and its severity, and better monitoring of H2S carry-over [1][2]. OSHA notes that weld hardness limits may not fully prevent cracking [1].

## Where integrity problems show up

| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Refinery vessels in wet H2S service | Water with H2S; hard zones at welds; no PWHT [1][2] | Internal WFMT of welds; ultrasonic testing for internal cracks [1][2][6] | [Hydrogen induced cracking](/glossary/hydrogen-induced-cracking/) |
| LPG storage spheres | H2S carry-over; as-welded, higher-strength steel [2] | WFMT; early inspection of spheres more than 5 years in service [1][2] | [Sulfide stress cracking](/glossary/sulfide-stress-cracking/) |
| Amine absorbers and vessels repaired without PWHT | Hard repair-weld zones; hydrogen [3][4] | Magnetic particle testing showed hundreds of weld cracks; ultrasonic testing showed internal separation [3] | [What is amine corrosion and amine cracking?](/library/amine-corrosion/) |
| Catalytic cracking overhead systems | Moist H2S with ammonia and cyanide from high-nitrogen feed [8] | Visual examination for blistering [1] | [What is fluid catalytic cracking (FCC)?](/library/fluid-catalytic-cracking/) |

Sources: OSHA Technical Manual, Section IV, Chapters 2 and 3 [1][8]; NIST SP 780, 1990 [2]; NIST SP 958 [3]; OSTI 403561 [6].

## Sources

1. [OSHA Technical Manual, Section IV, Chapter 3: Pressure Vessel Guidelines, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-3)
2. [NIST Special Publication 780, Guidelines for Pressure Vessel Safety Assessment (S. Yukawa), US National Institute of Standards and Technology (NIST)](https://nvlpubs.nist.gov/nistpubs/Legacy/SP/nistspecialpublication780.pdf)
3. [Analysis of the Catastrophic Rupture of a Pressure Vessel (prepared by T. Siewert), in NIST SP 958, A Century of Excellence in Measurements, Standards, and Technology, pp. 350-352, US National Institute of Standards and Technology (NIST)](https://nvlpubs.nist.gov/nistpubs/sp958-lide/html/350-352.html)
4. [Potentially Hazardous Amine Absorber Pressure Vessels Used in Refinery Processing (standard interpretation memorandum), US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/laws-regs/standardinterpretations/1986-04-11), 1986-04-11
5. [Research report on characterization and monitoring of cracking in wet H2S service (M. S. Cayard, R. D. Kane, L. Kaley, M. Prager), Welding Research Council Bulletin 396 (OSTI record 69967), US Department of Energy, Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/69967)
6. [Research report on ultrasonic characterization and monitoring of cracking in wet H2S service (OSTI record 403561), US Department of Energy, Office of Scientific and Technical Information (OSTI)](https://www.osti.gov/biblio/403561)
7. [Comparative Analysis of Ultrasonic NDT Techniques for the Detection and Characterisation of Hydrogen-Induced Cracking (R. J. Kazys, L. Mazeika, V. Samaitis, R. Sliteris, P. Merck, Z. Viliunas), Materials 15(13):4551, MDPI, via PubMed Central (open access, CC BY 4.0)](https://pmc.ncbi.nlm.nih.gov/articles/PMC9267232/), 2022-06-28
8. [OSHA Technical Manual, Section IV, Chapter 2: Petroleum Refining Processes, US Occupational Safety and Health Administration (OSHA)](https://www.osha.gov/otm/section-4-safety-hazards/chapter-2)