What are permanently installed ultrasonic thickness sensors?
Permanently installed ultrasonic thickness sensors are transducers fixed to a pipe or vessel wall that measure its thickness at a fixed spot on a schedule. Readings travel by cable or radio. Because position and coupling stay the same, the sensors track wall loss far more repeatably than hand-held surveys, but only where they are mounted.
By Jun Zhong, Editor·Researched and drafted by Beacon's AI newsroom·Checked by Jun Zhong, Editor·Last checked ·Next review
Why does it matter?
Fixing a thickness sensor in place makes its readings far more repeatable, but it does not make a single reading much more accurate, and it still sees only the spot beneath it 1. Hand-held ultrasonic readings taken months apart, often by different inspectors, are expected to scatter by about 0.25 to 1 mm because the probe never returns to exactly the same position with the same couplant 1. A 2015 Imperial College London thesis found that removing those errors and measuring often can cut the time needed to detect a corrosion rate of 0.1 mm per year (mm/y) to a few days 1. The trade-off is coverage: each sensor is a point measurement 3.
How do permanently installed sensors work?
The physics is the same as a hand-held gauge: the sensor times an ultrasonic pulse through the wall and back, and the travel time is converted to thickness with the speed of sound in the metal 1,3. See How does ultrasonic thickness measurement work? for the basic measurement. What changes is the mounting and the data path.
- Bonded strips and arrays. A 2003 report for the US Minerals Management Service (MMS) described thin, flexible strips carrying many ultrasonic elements, bonded permanently to an offshore riser to monitor a critical area 4.
- Waveguide transducers for hot surfaces. The thesis used a commercial design in which two thin metal strips, about 1 mm by 15 mm in cross-section, carry sound between the wall and piezoelectric elements kept away from the heat; one strip sends and the other receives 1.
- Electromagnetic acoustic transducers (EMATs). These generate sound inside the metal with a coil and a magnet, so they need no couplant and can work at elevated temperature 6.
- Wired or wireless data. Readings are taken automatically at set intervals 1. A 2019 review by researchers at the US National Energy Technology Laboratory (NETL) lists passive wireless sensors among emerging corrosion sensors and notes that electrically powered sensors in flammable atmospheres must meet intrinsic safety requirements 3. A 2024 laboratory study powered sensors wirelessly through coils from a hand-held reader, aiming at dense networks of measurement points in petrochemical plants 5.
The result is a thickness-versus-time trend whose slope is the wall loss rate. The thesis shows that the scatter of that slope depends on both the scatter of each reading and the spacing of readings: making the interval between readings four times longer doubles the slope's variability 1.
How repeatable and accurate are they?
| Reading type and conditions | Reported figure | Source |
|---|---|---|
| Hand-held readings in plants, repeated over time | Errors of about 0.25 to 1 mm expected | 1 |
| Hand-held digital gauge on riser steel in the field | Resolution 0.1 mm, accuracy about ±0.5 mm | 4 |
| Fixed sensor, laboratory, temperature stable within 0.1 °C | Standard deviation under 20 nm (0.00002 mm) | 1 |
| Fixed sensor, laboratory, 10 mm steel, over one day | Repeatability about 40 nm; loss rates of 0.1 to 0.2 mm/y detected within 1 to 2 hours | 2 |
| Fixed sensor, laboratory corrosion tests with temperature swings of about 4 °C | Wall loss of 1 µm detected reliably | 1 |
The fixed-sensor figures are laboratory results; the sources read do not give field accuracy for installed sensors. The thesis draws the key distinction: fixing the sensor improves repeatability (precision) by orders of magnitude, while the absolute accuracy of any one reading improves only marginally 1.
Three factors limit even fixed sensors 1:
- Temperature. It was the largest error source among those tested, because the speed of sound changes with temperature, so readings need compensation. 1
- Rough inner surfaces. Corrosion roughens the inner wall and distorts the echo. A cross-correlation method in the thesis cut wall-loss-rate errors by an order of magnitude; with it, 90% of measured rates fell within 7.5 ± 18% of the true slope, so a true 1 mm/y would read roughly 0.75 to 1.1 mm/y. 1
- Single sensor scatter. Combining several sensors on one area reduced the error to about 30% of a single sensor's variability. 1
Where are they used, and what limits them?
They suit spots that are hard to reach by hand. The thesis lists pipes that must be stripped of insulation, dug up or reached by scaffolding before a manual reading 1. The MMS report described bonded strips giving continuous readings at a critical riser area, but they needed coating removal and a clean, smooth surface 4. Frequent readings can also be lined up with process changes or inhibitor dosing 1.
The limits follow from the physics. Each sensor covers one spot. The NETL review makes a related point for coupons and ER probes: sites are usually chosen from experience, so unusual locations can be missed 3. Ultrasonic resolution depends on frequency and is often too coarse for small pits 3. Damage that weakens steel without thinning it, such as the small voids of high temperature hydrogen attack, does not show as wall loss; the thesis studied sound velocity changes as a possible indicator instead 1.
Where integrity problems show up
| What it finds well | What it can miss or get wrong | In the Library |
|---|---|---|
| Slow, general wall loss at the sensor, with laboratory repeatability in tens of nanometres 1,2 | Thinning a short distance away: each sensor is a point measurement, and fixed monitoring sites are usually picked from experience 3 | What are condition monitoring locations (CMLs)? |
| Changes in loss rate that can be matched to process changes or inhibitor dosing 1 | True loss under a rough, pitted inner surface, where distorted echoes bias standard processing 1; pits smaller than the frequency can resolve 3 | What is pitting corrosion? |
| Repeat readings at a critical riser area, from a bonded array strip 4 | Readings when temperature swings are not compensated, the largest error source in the thesis tests 1 | What are the main non-destructive testing (NDT) methods in oil and gas? |
| Wall thickness on hot surfaces, with waveguide or EMAT sensors 1,6 | Damage that does not thin the wall, such as hydrogen attack voids 1 | What is high temperature hydrogen attack (HTHA)? |
Sources: Gajdacsi, Imperial College London thesis, 2015 1; Zou and Cegla, 2017 2; Wright et al., NETL review, 2019 3; US Minerals Management Service riser report, 2003 4; NDE-Ed 6.
Common questions
- How is this different from an electrical resistance (ER) probe?
- An ER probe inserted into the process reports metal loss of its own sensing element. An ultrasonic sensor on the outside measures the remaining wall of the equipment itself. See [Electrical resistance probe](/glossary/electrical-resistance-probe/).
- Can they measure on hot pipe?
- Yes, with designs that keep the piezoelectric element cool, such as waveguide strips, or with EMATs, which need no couplant.
- How is it different from guided wave testing?
- Guided waves travel along the pipe for long distances and screen it for significant wall loss, while a thickness sensor measures through the wall at one spot. See [Guided wave testing](/glossary/guided-wave-testing/).
Beacon explains these concepts in its own words for education. It does not reproduce or replace the standards cited, and Winda is not affiliated with or endorsed by the organizations that publish them. Engineering decisions need the current edition of the standard and a qualified engineer.
Sources
- 1.High accuracy ultrasonic degradation monitoring (PhD thesis, A. Gajdacsi) · Imperial College London, Department of Mechanical Engineering (Spiral repository)
- 2.High Accuracy Ultrasonic Corrosion Rate Monitoring (F. Zou, F. B. Cegla), Corrosion, doi 10.5006/2586 (abstract, accepted manuscript record) · Imperial College London (Spiral repository); journal published by NACE International, now AMPP ·
- 3.Corrosion Sensors for Structural Health Monitoring of Oil and Natural Gas Infrastructure: A Review (R. F. Wright et al.), Sensors 19(18):3964 · MDPI, via PubMed Central (authors at the US National Energy Technology Laboratory) ·
- 4.Evaluation of Methods for Detecting and Monitoring of Corrosion and Fatigue Damage in Risers (M. Lozev, B. Grimmett, E. Shell, R. Spencer), final report, Technical Assessment Program project 433 · US Minerals Management Service (now Bureau of Safety and Environmental Enforcement, BSEE) ·
- 5.Research on Wireless Passive Ultrasonic Thickness Measurement Technology Based on Pulse Compression Method (L. Pan et al.), Sensors 24(24):8023 · MDPI, via PubMed Central ·
- 6.Electromagnetic Acoustic Transducers (EMATs) (NDE-Ed) · Iowa State University, Center for Nondestructive Evaluation