Skip to content
Beaconby Winda
FactCorrosion and Damage Mechanisms · Environmental cracking

Sensitization

·2 sources

Short answer

Sensitization is the formation of chromium carbides along the grain boundaries of austenitic stainless steel heated in a certain temperature band.

By , Editor·Researched and drafted by ·Checked by , Editor·Last checked

The carbides drain chromium from the adjacent metal, and these thin chromium-depleted zones lose their passive film and become preferred paths for intergranular corrosion and cracking 1. A 2026 review puts the main band at about 500 to 800 °C (930 to 1,470 °F), reached for example during welding or heat treatment 1. US tank car rules require Type 304L and 316L test samples to receive a deliberate "sensitizing treatment", typically 1 hour at 1,250 °F (about 677 °C), before an intergranular attack test (49 CFR 179.200-7(d)) 2.

Heat pulls chromium, the element that keeps stainless steel from rusting, out of the metal along grain edges, which can then corrode or crack while the grains themselves stay protected. Stabilized grades resist it: in AISI 347, added niobium ties up the carbon, which delays carbide formation to higher temperatures 1.

Sources

  1. 1.Understanding failure in austenitic steels: Key considerations for molten salt storage in CSP applications (S. A. Ardila-Parra, C. Prieto, J. D. Osorio, A. I. Fernández, Journal of Materials Research and Technology 41, 7378 to 7398) · US Department of Energy, Office of Scientific and Technical Information (OSTI), full text ·
  2. 2.49 CFR 179.200-7, Materials (tank cars) · eCFR, US Office of the Federal Register