What are a welding procedure specification (WPS) and a procedure qualification record (PQR)?
A welding procedure specification (WPS) is the written instruction that sets how a production weld is made and the limits welders must work within. A procedure qualification record (PQR) documents the test weld and results that prove the WPS works. Welders are qualified separately. ASME Section IX, AWS B2.1 and API Std 1104 set the rules.
By Jun Zhong, Editor·Researched and drafted by Beacon's AI newsroom·Checked by Jun Zhong, Editor·Last checked ·Next review
Why does it matter?
A qualified welding procedure does not show that the person welding is qualified: US gas pipeline rules require qualified procedures in one section and qualified welders in another 1,2. The same rules require the test welds behind a procedure to be judged by destructive testing, and each procedure to be recorded in detail with its test results, kept and followed whenever it is used 1,3. A 1990 assessment by the US National Institute of Standards and Technology (NIST) notes that ASME Section VIII likewise requires a written WPS and qualified procedures and welders, to keep the vessel's margin against failure 9.
What does a WPS contain?
A WPS tells welders and inspectors which process, materials and settings to use, within ranges a test has shown to work; the rules in AWS B2.1 cover base metals, filler metals, qualification variables, joint designs and testing 6. Typical content:
- Process and technique, such as shielded metal arc or gas tungsten arc, and whether welding is manual, semiautomatic, mechanized or automatic 6.
- Base metal, filler metal and joint design 6.
How is a welding procedure qualified?
- Weld a test piece with it and record the conditions actually used 1.
- Test the test piece. US pipeline rules require test welds for procedure qualification to be judged by destructive testing 1,3.
- Record the results. The detailed record with the qualifying test results is the PQR, which must be retained 1,3; ISO-based standards call it a welding procedure qualification record (WPQR).
- Issue the WPS with production ranges that the PQR supports 7.
Some routes avoid a company's own test. AWS publishes Standard Welding Procedure Specifications (SWPSs), each backed by at least two PQRs and with ranges narrower than AWS B2.1 allows 7.
How are welders qualified?
Welder qualification tests whether a person can make an acceptable weld while following a procedure; AWS calls it performance qualification 6. US pipeline rules add detail:
- Welders and welding operators must qualify under API Std 1104 or ASME Section IX 2,4; gas rules allow a simpler test for pipe operating at a hoop stress below 20% of specified minimum yield strength 2.
- On hazardous liquid lines, nobody may weld with a process unless, in the previous 6 calendar months, they used that process and had a weld tested and accepted 4.
- For steel gas transmission pipe installed after 1 July 2021, records of each welder's qualification at construction must be kept for at least 5 years 2.
Which codes govern WPS, PQR and welder qualification?
| Document | Publisher | Where it is used | Edition (publisher page) |
|---|---|---|---|
| BPVC Section IX, Welding, Brazing, and Fusing Qualifications | ASME | Qualification of procedures required by other ASME code sections; one of two routes named in US pipeline rules 1,5 | 2025 5 |
| B2.1/B2.1M, Specification for Welding Procedure and Performance Qualification | AWS | Procedures, welders and welding operators for 12 welding processes 6 | 8th edition, 2026 6 |
| Std 1104, Welding of Pipelines and Related Facilities | API | Carbon and low-alloy steel pipeline welding, new and in service, with inspection and acceptance standards; the other route in US pipeline rules 1,8 | 22nd edition, July 2021 8 |
| RP 582, Welding Guidelines for the Chemical, Oil, and Gas Industries | API | Supplementary guidance for pressure equipment, tanks and attachments, in shop and field 8 | 4th edition, May 2023 8 |
API editions as listed in API's 2025 catalog 8.
Where integrity problems show up
| Decision or step at this stage | What it affects later | In the Library |
|---|---|---|
| Qualifying a procedure without the PWHT or hardness control the service needs | Cracking at as-welded or hard welds in amine and wet hydrogen sulfide service 10 | What is amine corrosion and amine cracking? |
| Welding equipment for hydrogen sulfide production service | US offshore rules require such welding to be minimized and done so welds resist sulfide stress cracking 11 | Sulfide stress cracking |
| Using welders who are unqualified or out of practice | Weld defects; NIST lists undetected weld defects among construction-stage causes of later failures 9 | How is fabrication quality controlled for pressure equipment? |
| Not keeping WPS, PQR and welder records | Procedure records must be kept and followed 1,3; OSHA lists weld examination and PWHT details among information for in-service safety assessment 10 | What is weld mapping and weld traceability? |
| Planning repair welds | NIST notes that the repair codes it reviewed require qualified welders and generally PWHT in cracking-prone service 9 | What is API 510? |
Sources: 49 CFR 192.225 1 and 195.214 3; NIST, 1990 9; OSHA 10; 30 CFR 250.490 11.
Common questions
- What is the difference between a WPS and a PQR?
- The WPS is the instruction used in production, with ranges for each variable. The PQR is the record of the test weld behind it, with the values actually used and the test results.
- Can one company use another company's WPS?
- It depends on the code and contract; the ASME, AWS and ISO routes above differ.
- Is a WPS required by law?
- For US gas and hazardous liquid pipelines, yes: welding must follow qualified procedures. For pressure vessels, ASME Section VIII requires a WPS, and NIST notes the code gains legal force where a jurisdiction adopts it.
Beacon explains these concepts in its own words for education. It does not reproduce or replace the standards cited, and Winda is not affiliated with or endorsed by the organizations that publish them. Engineering decisions need the current edition of the standard and a qualified engineer.
Sources
- 1.49 CFR 192.225, Welding procedures · eCFR, US Office of the Federal Register
- 2.49 CFR 192.227, Qualification of welders and welding operators · eCFR, US Office of the Federal Register
- 3.49 CFR 195.214, Welding procedures · eCFR, US Office of the Federal Register
- 4.49 CFR 195.222, Welders and welding operators: Qualification of welders and welding operators · eCFR, US Office of the Federal Register
- 5.BPVC.IX, BPVC Section IX, Welding, Brazing, and Fusing Qualifications (product page) (2025) · American Society of Mechanical Engineers (ASME)
- 6.AWS B2.1/B2.1M:2026, Specification for Welding Procedure and Performance Qualification (preview: title page, abstract, foreword) (8th edition, 2026) · American Welding Society (AWS)
- 7.Standard Welding Procedure Specifications (SWPS) (committee page) · American Welding Society (AWS)
- 8.2025 Publications Catalog (entries for Std 1104 and RP 582) · American Petroleum Institute (API)
- 9.NIST Special Publication 780, Guidelines for Pressure Vessel Safety Assessment (S. Yukawa) · US National Institute of Standards and Technology (NIST)
- 10.OSHA Technical Manual, Section IV, Chapter 3: Pressure Vessel Guidelines · US Occupational Safety and Health Administration (OSHA)
- 11.30 CFR 250.490, Hydrogen sulfide · eCFR, US Office of the Federal Register