What is carbon dioxide (CO2) corrosion?
Carbon dioxide (CO2) corrosion, or sweet corrosion, is metal loss on carbon and low-alloy steel caused by CO2 dissolving in water to form carbonic acid. Dry CO2 does not corrode steel. It affects wells, flowlines and pipelines carrying wet gas or produced water; US pipeline rules (49 CFR 192.475, 195.579) require operators to investigate and limit it.
By Jun Zhong, Editor·Researched and drafted by Beacon's AI newsroom·Checked by Jun Zhong, Editor·Last checked ·Next review
Why does it matter?
Hotter is not always faster. In Ohio University tests on carbon steel in CO2-saturated brine at high pressure, the rate was about 10 mm per year (mm/y) at 65 °C, but at 90 °C it fell to about 0.05 mm/y once a protective iron carbonate layer had formed 1. At 65 °C the surface carried only patches of porous iron carbide, which gave no protection 1. Because so much depends on whether that layer forms and stays, CO2 corrosion rates are set by temperature, water chemistry, flow and steel type, not by CO2 content alone 1,2.
How does CO2 corrosion happen?
When it meets liquid water it dissolves and forms carbonic acid, a weak acid that partly splits into bicarbonate and carbonate ions 6. Iron dissolves at the steel surface while hydrogen ions are reduced, and the result can be uniform thinning or local attack 2,6.
As iron goes into solution, iron carbonate can precipitate on the surface. A dense layer slows the transport of reacting species to the steel, while the iron carbide skeleton left behind by corrosion is porous and does not protect 1,2. Studies of this mechanism go back at least to work by de Waard and Milliams in 1975 2.
What controls the rate of CO2 corrosion?
- Gas composition. The amount of CO2 matters, as do hydrogen sulfide (H2S), oxygen, sulfur oxides and nitrogen oxides, which dissolve in the water and lower its pH 6.
- Water chemistry and pH. Acidic water (pH below 7) is generally more corrosive to carbon steel than basic water 3.
- Temperature and surface layers. Temperature decides whether a protective iron carbonate layer forms; tests showed the rate dropping by more than 99% between 65 and 90 °C under one set of conditions 1.
- Flow. In multiphase lines carrying oil, gas and salt water together, the transfer of species to and from the wall and the thickness of the corrosion product layer both govern the rate 2.
- Material. Corrosion-resistant alloys are an option for severe service, but carbon and low-alloy steels remain widely used for tubing because of strength, availability and cost 1.
How is CO2 corrosion found?
Internal corrosion in a gas pipeline can be found by examining the inside of pipe when it is opened, measuring wall thickness from the outside, reading corrosion coupons or probes placed in the line, or running an in-line inspection tool 3. Sampling the gas and the liquids and solids removed from the line shows whether corrosive water and contaminants are present 3.
US rules turn some of this into requirements. Wherever pipe is removed from a gas or hazardous liquid line, its inside surface must be inspected for corrosion 4,5. Where corrosive gas is carried, coupons or other monitoring must be checked twice each calendar year, at intervals of no more than 7.5 months 4. Where inhibitors protect a hazardous liquid or CO2 line, coupons or other monitoring must show whether they work 5.
How is CO2 corrosion controlled?
- Keep water out or remove it. Controlling the quality of gas entering a pipeline and removing liquids reduce the chance of corrosion; at Carlsbad, New Mexico, investigators found that regular cleaning pigs with full removal of liquids would likely have made the corrosion less severe 3. Dewatering is a central control for CO2 transport pipelines 6.
- Design out water traps. Since 2007, new and replaced US onshore gas transmission lines must be configured to limit liquid collection, have liquid removal features where liquids can collect, and allow corrosion monitoring devices at likely locations 4.
- Inject inhibitors. Inhibitors are often injected into carbon steel lines carrying wet gas or process brines 7; US liquid and CO2 line rules require enough inhibitor to protect the whole section it is meant for 5.
- Select alloys. Corrosion-resistant alloys avoid the problem where carbon steel cannot be protected economically 1.
Where integrity problems show up
| Where it occurs (unit or equipment) | Conditions that drive it | How it is usually found | In the Library |
|---|---|---|---|
| Low points, sags and drips in gas pipelines | Water with CO2, chlorides, oxygen, H2S and microbes collecting where cleaning pigs could not run; NTSB found this combination likely caused the 2000 Carlsbad rupture 3 | In-line inspection, external wall thickness measurement, coupons or probes, sampling of removed liquids 3 | What is in-line inspection (ILI) and pigging? |
| Pipelines carrying corrosive gas | CO2 and free water 4 | Coupons or other monitoring checked twice a year 4 | Corrosion coupons vs electrical resistance (ER) probes |
| New and replaced onshore gas transmission lines | Configurations that let liquids collect 4 | Monitoring devices built in at locations with significant potential for internal corrosion 4 | What is corrosion monitoring and which methods are used? |
| CO2 pipelines for capture and storage | Water dropping out of dense-phase CO2; oxygen, sulfur and nitrogen oxides, H2S 6 | Coupons or other monitoring where inhibitors are used 5 | How are carbon dioxide pipelines different from natural gas pipelines? |
| Carbon steel production tubing in high-CO2 deep-water wells | High CO2 pressure and brine at temperatures where iron carbonate does not protect 1 | Laboratory qualification by weight loss and linear polarization resistance before selection 1 | What is linear polarization resistance (LPR) monitoring? |
Sources: NTSB/PAR-03/01, 2003 3; 49 CFR 192.475 to 192.477 4; 49 CFR 195.579 5; Choi et al., 2014 1; Liu et al., 2025 6.
Common questions
- What is the difference between sweet and sour corrosion?
- Sweet corrosion is attack driven by CO2 dissolved in water. Sour corrosion involves hydrogen sulfide instead; a sour brine is one contaminated by H2S.
- Is dry CO2 corrosive?
- No. Dry CO2, as gas or supercritical fluid, does not corrode steel; the problem starts when free water is present.
- Can CO2 corrosion rates be predicted?
- Mechanistic models combine water chemistry, CO2 dissolution, mass transfer, surface reactions and the corrosion product layer; one 1998 model of this kind matched its experimental results well. Predictions still depend on knowing where water will collect.
Beacon explains these concepts in its own words for education. It does not reproduce or replace the standards cited, and Winda is not affiliated with or endorsed by the organizations that publish them. Engineering decisions need the current edition of the standard and a qualified engineer.
Sources
- 1.Corrosion Behavior of Deep Water Oil Production Tubing Material Under Supercritical CO2 Environment: Part 1, Effect of Pressure and Temperature (Y.-S. Choi et al.), Corrosion 70(1) · NACE International; copy hosted by the Institute for Corrosion and Multiphase Technology, Ohio University
- 2.Modeling the Diffusion Effects through the Iron Carbonate Layer in the Carbon Dioxide Corrosion of Carbon Steel (S. Rajappa, R. Zhang, M. Gopal), Paper No. 26 · NACE International; copy hosted by Ohio University
- 3.Natural Gas Pipeline Rupture and Fire Near Carlsbad, New Mexico, August 19, 2000 (NTSB/PAR-03/01) · US National Transportation Safety Board (NTSB) ·
- 4.49 CFR 192.475, 192.476 and 192.477, Internal corrosion control · eCFR, US Office of the Federal Register
- 5.49 CFR 195.579, What must I do to mitigate internal corrosion? (and definitions in 195.2) · eCFR, US Office of the Federal Register
- 6.Research Progress on Major Influencing Factors of Corrosion Behavior of Pipeline Steel in Supercritical CO2 Environment (Z. Liu et al.), Materials 18(11) · MDPI (open access, CC BY), via PubMed Central ·
- 7.Bimetallic Corrosion (Guides to Good Practice in Corrosion Control No. 5) · UK National Physical Laboratory (NPL)