What is corrosion monitoring and which methods are used?
Corrosion monitoring is the repeated or continuous measurement of corrosion rate, or of how corrosive a process stream is, over time. Common tools are coupons, electrical resistance (ER) and linear polarization resistance (LPR) probes, fixed ultrasonic sensors and fluid sampling. US pipeline rules (49 CFR 192.477 and 195.579) require coupons or equivalent monitoring for corrosive gas and inhibitor programs.
By Jun Zhong, Editor·Researched and drafted by Beacon's AI newsroom·Checked by Jun Zhong, Editor·Last checked ·Next review
Why does it matter?
On August 19, 2000, a 30-inch natural gas transmission pipeline ruptured beside the Pecos River near Carlsbad, New Mexico; the gas ignited and 12 people camping nearby were killed 1. Internal corrosion had removed up to 72% of the original wall along the bottom of the pipe 1. The National Transportation Safety Board (NTSB) reported that no corrosion coupons or monitoring devices were used on that section, because company officials did not believe the gas was corrosive 1. It found that monitoring the gas entering the line and sampling the liquids and solids removed from it would likely have shown the potential for serious corrosion 1.
How is corrosion monitoring different from inspection?
A 2019 review by researchers at the US National Energy Technology Laboratory (NETL) sorts corrosion sensors into direct ones, which follow the corrosion process or rate, and indirect ones, which follow its causes, such as water, pH and carbon dioxide, or its results, such as wall loss 4. Coupons and probes sit in the process at chosen points and report what happens to a metal sample there 4. Inspection, by contrast, measures the equipment wall itself; see How does ultrasonic thickness measurement work? and What is in-line inspection (ILI) and pigging?.
Which methods are used?
| Method | What it measures | How often it gives a result | Main limits |
|---|---|---|---|
| Weight-loss coupon | Metal lost from a sample during an exposure period 4 | After retrieval and laboratory analysis; the NETL review gives a few months 4 | Average rate only, no real-time data, one location 4 |
| Electrical resistance (ER) probe | Rise in the resistance of a metal element as it thins; gives cumulative metal loss, from which a rate is inferred 4,5 | Continuously or at intervals, without removing the probe 5 | Common elements track uniform corrosion; one location; electrical safety rules apply in flammable areas 4 |
| Linear polarization resistance (LPR) probe | Electrochemical estimate of the instantaneous corrosion rate 5 | Within minutes 5 | Needs a conductive, usually water-based, liquid; may need calibration against other methods; the applied signal can raise the measured rate 4,5 |
| Fixed ultrasonic sensors | Wall thickness of the equipment at the sensor 7 | Repeated readings for trending 7 | Covers a local area only 7 |
| Gas and liquid sampling | Corrosive agents in the stream, such as water, chlorides, oxygen, carbon dioxide, hydrogen sulfide and microbes 1 | Each sample 1 | Shows corrosivity, not metal loss on the equipment 4 |
Sources: Wright et al., 2019 4; ASTM G96 product page 5; US Minerals Management Service report, 2003 7; NTSB/PAR-03/01 1.
Where are monitoring points placed?
The NETL review notes that coupon and probe locations have to be picked for each system, usually from experience, and that unusual locations with heavy corrosion can be left out 4. At Carlsbad, liquids that bypassed a partly clogged liquid trap collected at a low point formed by a pipe bend, which is where the pipe corroded 1. US rules set a minimum check frequency: coupons or other monitoring means on corrosive gas lines, and on liquid lines using inhibitors, must be checked at least twice each calendar year at intervals of no more than 7.5 months 2,3.
How are the results used?
- Early warning. ASTM's public scope text for its online monitoring guide (G96) describes ER and polarization methods as a way to catch corrosive conditions from process upsets before significant damage 5.
- Inhibitor control. A rising measured rate can show that more inhibitor is needed 5; US liquid pipeline rules require coupons or other monitoring to judge whether inhibitors work 3.
- Integrity management. US gas transmission operators must bring results from gas sampling, internal corrosion monitoring and cleaning pig samples into their threat and risk assessment 6.
Where integrity problems show up
| What it finds well | What it can miss or get wrong | In the Library |
|---|---|---|
| Changes in corrosivity after process upsets, read without removing ER or LPR probes, LPR within minutes 5 | Corrosion away from the probe; coupons and probes are point sensors 4 | Online vs offline corrosion monitoring |
| The average corrosion rate of the sample over its exposure 4 | Short corrosive episodes averaged out over months of exposure 4,5 | Corrosion coupons vs electrical resistance (ER) probes |
| Uniform metal loss on ER elements 4 | Pitting and other local attack on common ER elements 4 | What is pitting corrosion? |
| Corrosive agents in gas and liquids, including microbes 1 | Corrosion where nobody samples or monitors: the section that failed at Carlsbad in 2000 had neither coupons nor monitoring devices 1 | What is microbiologically influenced corrosion (MIC)?, What is carbon dioxide (CO2) corrosion? |
| Wall thinning trend at a critical spot, with fixed ultrasonic sensors 7 | Thinning outside the sensor's local area 7 | What are permanently installed ultrasonic thickness sensors? |
Sources: NTSB/PAR-03/01, 2003 1; Wright et al., 2019 4; ASTM G96 product page 5; US Minerals Management Service report, 2003 7.
Common questions
- How often must coupons be checked under US pipeline rules?
- At least twice each calendar year, with no more than 7.5 months between checks, for gas lines carrying corrosive gas and for hazardous liquid lines that rely on inhibitors.
- What is the difference between online and offline monitoring?
- Online methods such as ER and LPR read metal loss or corrosion rate without removing the probe, while coupons must be withdrawn from the system to be evaluated. See [Online vs offline corrosion monitoring](/library/online-vs-offline-monitoring/).
- Is a corrosion monitoring point the same as a condition monitoring location (CML)?
- No. A CML is a marked spot on the equipment wall that inspectors measure, while a coupon or probe measures a sample in the process.
Beacon explains these concepts in its own words for education. It does not reproduce or replace the standards cited, and Winda is not affiliated with or endorsed by the organizations that publish them. Engineering decisions need the current edition of the standard and a qualified engineer.
Sources
- 1.Pipeline Accident Report: Natural Gas Pipeline Rupture and Fire Near Carlsbad, New Mexico, August 19, 2000 (NTSB/PAR-03/01) · US National Transportation Safety Board (NTSB)
- 2.49 CFR 192.477, Internal corrosion control: Monitoring · eCFR, US Office of the Federal Register
- 3.49 CFR 195.579, What must I do to mitigate internal corrosion? · eCFR, US Office of the Federal Register
- 4.Corrosion Sensors for Structural Health Monitoring of Oil and Natural Gas Infrastructure: A Review (R. F. Wright et al.), Sensors 19(18):3964 · MDPI, via PubMed Central ·
- 5.ASTM G96-90(2018), Standard Guide for Online Monitoring of Corrosion in Plant Equipment (Electrical and Electrochemical Methods) (product page, Scope and Significance) (G96-90 (reapproved 2018), marked historical on the ASTM store) · ASTM International
- 6.49 CFR 192.917, How does an operator identify potential threats to pipeline integrity and use the threat identification in its integrity program? · eCFR, US Office of the Federal Register
- 7.Evaluation of Methods for Detecting and Monitoring of Corrosion and Fatigue Damage in Risers (M. Lozev et al.), Technical Assessment Program project 433 · US Minerals Management Service (now Bureau of Safety and Environmental Enforcement, BSEE) ·