Skip to content
Beaconby Winda
FactCorrosion and Damage Mechanisms · High-temperature damage

What is high-temperature oxidation?

·9 sources

Short answer

High-temperature oxidation is the reaction of a metal with oxygen in hot air, flue gas or steam, which grows an oxide scale on its surface. A thin, adherent scale slows further attack; thick or flaking scale thins the wall and hinders heat transfer. Alloys richer in chromium form more protective scales.

By , Editor·Researched and drafted by ·Checked by , Editor·Last checked ·Next review

Why does it matter?

A 2014 model from Oak Ridge National Laboratory (ORNL) predicted that oxide scale flaking from the steam side of stainless steel superheater tubes could block more than half of a tube bend within the first two years of boiler operation, at outlet tube temperatures of 540 to 570 °C (about 1,000 to 1,060 °F) 3. The authors noted that this matched practical experience 3. A blocked tube is starved of steam and can overheat: boiler failure reports reviewed by Basson and Fuls (2021) found short-term overheating caused by oxide scaling most often in horizontal superheaters 6. A thin, adherent scale protects the metal; the problems start when scale grows thick or breaks away 1,2.

How does a metal oxidize at high temperature?

When hot metal meets oxygen, the two react at the surface and build a solid oxide layer, called scale 1,2. Once the scale covers the surface, the reaction can continue only as metal or oxygen ions move through it, so the scale itself sets the pace 2. Most cases follow one of three rate laws: linear, where the rate stays constant because a surface reaction, not the scale, controls it; parabolic, where growth slows with time because diffusion through a thickening scale controls it; and logarithmic, which applies to very thin films 2.

Temperature has a strong effect. The UK National Physical Laboratory (NPL) gives a rule of thumb that, for many oxidation reactions, a change of 20 °C (36 °F) changes the oxidation rate about tenfold 1. Polluted hot gases, such as sulfur oxides, chlorine compounds and nitrogen oxides, can speed the attack further 1.

Which metals resist it?

Resistance rises with chromium, which helps form a tight, adherent chromium oxide scale 4. Work at Argonne National Laboratory (ANL) in hot, carbon-rich reformer gas found chromium oxide the most protective scale on commercial alloys 5.

NPL's checklist gives approximate temperatures below which oxidation in air is negligible: about 480 °C (about 900 °F) for mild steel, about 900 °C (about 1,650 °F) for grade 316 stainless steel and about 1,150 °C (about 2,100 °F) for a 25% chromium, 20% nickel stainless steel 1. NPL adds that creep strength or polluted gases can set lower practical limits 1; see What is creep damage?.

What damage does it cause?

  • Metal loss. Scale grows by consuming metal, so the wall gets thinner 1,2.
  • Overheating. Scale and deposits slow heat transfer more as they thicken, and NPL notes that thick scale and metal loss lead to overheating when tubes lose their cooling 1.
  • Spalling and blockage. Oxide takes up more volume than the metal it replaces, which stresses the scale; in laboratory tests the scale on pure iron ballooned and separated from the metal on cooling 2. ORNL modeling predicted that the earliest scale failures in superheater tubes would come from strains during boiler shutdowns, and the flakes can block tube bends 7,3.
  • Opening the way to other damage. In ethylene cracking tubes, carburization starts where the oxide scale spalls 4. In steam reformer tubes, oxidation of the inner surface changes thermal stress and creep damage 8.

How is it found?

  • Thickness, dimensions and surface condition. A 1994 field method for ethylene furnace tubes combined dimension and thickness measurements, visual inspection and surface replicas with electromagnetic instruments to assess oxidation and carburization together 9.
  • Prediction for steam-side scale. ORNL's models estimate scale growth, flaking and the share of a tube bend likely to be blocked, as a function of operating time and steam temperature 3,7.
  • After a failure. Blockage often comes to light when a tube overheats and ruptures 6; see What is short-term overheating of heater tubes?.

Where integrity problems show up

Where it occurs (unit or equipment)Conditions that drive itHow it is usually foundIn the Library
Boiler superheater and reheater tubesSteam-side scale grows, then flakes during shutdowns and collects in bends 3,7Scale growth and blockage modeling; often found after a tube overheats 3,6What is short-term overheating of heater tubes?
Ethylene cracking furnace tubesOxidation alongside carburization at very high wall temperatures 9Thickness and dimension checks, visual inspection, replicas and electromagnetic surveys 9What is a petrochemical plant?
Cast heat-resistant coils where scale spallsBare metal exposed to carbon-rich process gas 4Magnetic response of carburized metal 4What is carburization?
Steam reformer tubesInner-surface oxidation changes thermal stress and creep 8Full-length eddy current with laser deformation measurement 8What is creep damage?
Tubes heated by hot gasThick scale and metal loss raise metal temperature 1Wall thickness measurement 9How does ultrasonic thickness measurement work?

Sources: NPL, 2020 1; ORNL, 2011 and 2014 3,7; Saori and Ohta 4; Basson and Fuls, 2021 6; HIAD record of the 2018 KHK case 8; Lin and others, 1994 9.

Common questions

Is high-temperature oxidation the same as rusting?
No. NPL notes that ordinary corrosion needs a liquid phase, while at high enough temperatures a metal reacts directly with oxygen and forms scale. See [What is corrosion?](/library/corrosion/).
Does stainless steel oxidize?
Yes, once it is hot enough. NPL puts the limit for negligible oxidation of grade 316 stainless steel in air at about 900 °C.
How is it different from sulfidation?
Sulfidation is high-temperature attack by sulfur compounds rather than by oxygen; NPL notes that sulfurous flue gases speed up high-temperature attack. See [What is sulfidation (high-temperature sulfur corrosion)?](/library/sulfidation/).

Beacon explains these concepts in its own words for education. It does not reproduce or replace the standards cited, and Winda is not affiliated with or endorsed by the organizations that publish them. Engineering decisions need the current edition of the standard and a qualified engineer.

Sources

  1. 1.Corrosion control checklist (Guides to Good Practice in Corrosion Control No. 11) · UK National Physical Laboratory (NPL)
  2. 2.High-Temperature Oxidation of Metals (S. Samal), book chapter, DOI 10.5772/63000 · IntechOpen (open access) ·
  3. 3.Managing Oxide Scale Exfoliation in Boilers with TP347H Superheater Tubes (A. S. Sabau, I. G. Wright, J. P. Shingledecker, P. F. Tortorelli), conference paper (record and abstract) · Oak Ridge National Laboratory, via US DOE Office of Scientific and Technical Information (OSTI)
  4. 4.Carburization and its prevention in ethylene cracking furnace tubes (M. Saori, S. Ohta), TMS Paper Selection vol. 56 (record and abstract) · US DOE Office of Scientific and Technical Information (OSTI)
  5. 5.Argonne National Laboratory Develops Alloys to Resist Metal Dusting (fact sheet) · US Department of Energy, Industrial Technologies Program
  6. 6.Over-attemperation and Short-term Overheating in Pendant-type Superheaters (N. Basson, W. F. Fuls), R&D Journal of the South African Institution of Mechanical Engineering 37, 58-69 · South African Institution of Mechanical Engineering (open access, CC BY 4.0)
  7. 7.Steam-Side Oxide Scale Exfoliation Behavior in Superheaters and Reheaters (A. S. Sabau, J. P. Shingledecker, I. G. Wright), conference paper (record and abstract) · Oak Ridge National Laboratory, via US DOE Office of Scientific and Technical Information (OSTI)
  8. 8.Process gases leak in a reformer tube (HIAD 2.0 incident record, based on KHK accident database incident 2018-428) · Clean Hydrogen Partnership, Clean Hydrogen Knowledge Hub (European Union)
  9. 9.The field measurement of carburization and oxidation of ethylene furnace tubes by multi-technique method (J. Y. Lin, F. C. Chiang, H. Chang, C. C. Su) (record and abstract) · US DOE Office of Scientific and Technical Information (OSTI)