What is flue gas dew point corrosion?

·9 sources

Short answer

Flue gas dew point corrosion is attack on the coldest metal in a boiler or fired heater flue gas path when acid condenses from the gas onto it. Sulfuric acid formed from fuel sulfur is the usual cause. It hits economizers, air preheaters and stacks, and the metal temperature, not the gas temperature, decides where.

By , Editor·Researched and drafted by ·Checked by , Editor·Last checked ·Next review

Why does it matter?

Cooling flue gas further recovers more heat: the US Department of Energy (DOE) notes that boiler efficiency can generally rise by about 1% for every 40 °F (22 °C) drop in flue gas temperature 1. Yet DOE also sets a floor. It puts the coolest practical flue gas at about 250 °F (121 °C) for natural gas, 300 °F (149 °C) for coal and low-sulfur fuel oils and 350 °F (177 °C) for high-sulfur fuel oils, limits chosen to prevent condensation and possible stack corrosion 1. Condensing economizers go below that floor on purpose and can lift overall boiler efficiency above 90%, but they must be designed to withstand corrosion from the condensed water 2.

How does acid form in flue gas?

Sulfur in the fuel burns mostly to sulfur dioxide. For fuel oil, the US Environmental Protection Agency (EPA) reports that on average more than 95% of the sulfur becomes sulfur dioxide, about 1% to 5% is oxidized further to sulfur trioxide, and 1% to 3% leaves as sulfate particles 3. Sulfur trioxide reacts readily with water vapor in flue gas to form sulfuric acid mist 3. When metal in the gas path is cold enough, that acid condenses on it as a liquid film.

Water itself condenses at a much lower temperature. DOE gives the water dew point of natural gas combustion products as about 135 °F (57 °C) 9, well below its 250 °F (121 °C) minimum flue gas temperature for natural gas 1.

Sulfuric acid is not the only corrosive that can condense from flue gas 4,5,2:

  • Nitrogen oxides. When high-nitrogen crude is processed, nitrogen oxides can form in furnace flue gas; OSHA notes they attack steel once the gas is cold enough for water to be present 4.
  • Chlorides and ammonia. In boilers burning biomass or waste, flue gas carrying both hydrogen chloride and unreacted ammonia can deposit ammonium chloride at the cold end. The salt is hygroscopic and corroded carbon steel in tests even at humidity below the point where it fully dissolves 5.
  • Condensed water. Water condensed from burning natural gas or light oil is acidic; with oil it is more acidic because of dissolved sulfur oxides 2.

Where does dew point corrosion occur?

The attack happens wherever metal sits below the acid dew point, and that depends on the metal temperature more than the bulk gas temperature 6. A 2024 study of a damaged air preheater in a boiler fired with a gas mixture, by researchers at Cracow University of Technology, found sulfuric acid solution running down the vertical air heater tubes and corroding them and the water heater tubes below, which were perforated 6. Cold incoming air lowered tube temperatures, and an abrupt widening of the air duct sent air unevenly through the bundle, leaving colder zones 6. The authors named too-deep cooling of the flue gas as the root cause and noted that corrosion is most likely during low or changing load, start-ups and shutdowns 6.

DOE's process heating guidance makes the same point for heat recovery in general: when low-temperature waste gas is cooled, condensing water vapor or other condensables can corrode the recovery equipment 7.

How is dew point corrosion prevented and found?

  • Keep surfaces above the limit. DOE's first steps for an economizer project are to measure the stack temperature and to set the lowest temperature the gas can be cooled to, given dew point and cold-end corrosion 1.
  • Lower the dew point at the source. The 2024 study recommended removing sulfur trioxide while the gas is still in the furnace, so the dew point falls and corrosive conditions do not arise, and correcting the air duct design 6.
  • Design for condensation where it is intended. Condensing economizers need special corrosion-resistant materials or coatings, and their acidic condensate is neutralized before it is discharged or reused 2.
  • Inspect. API RP 573, Inspection of Fired Boilers and Heaters (4th edition, January 2021), covers inspection practices for boilers and process heaters in refineries and petrochemical plants, including the on-stream and off-stream data needed to judge their condition 8. In the 2024 case, damage was found as perforated tubes, and computer flow modeling then traced the cold zones 6.

Where integrity problems show up

Where it occurs (unit or equipment)Conditions that drive itHow it is usually foundIn the Library
Boiler economizer outlet and stackFlue gas cooled below the fuel's minimum: about 250, 300 or 350 °F 1Stack temperature measured against the limit for the fuel 1What is a fired heater?
Air preheater tubes at the cold endCold incoming air, uneven airflow, low load, start-ups, shutdowns 6Perforated tubes; flow modeling to locate cold zones 6What are the main types of heat exchangers in process plants?
Condensing economizersGas cooled below the water dew point by design; acidic condensate, more so with oil 2Condensate handled as acidic and neutralized before discharge or reuse 2What are corrosion-resistant alloys (CRAs)?
Crude unit furnace flue gas pathNitrogen oxides from high-nitrogen crude, cooled in the presence of water 4On-stream and off-stream inspection practices in API RP 573 8What is a crude distillation unit?

Sources: DOE Steam Tip Sheets #3 and #26B, 2012 1,2; OSHA Technical Manual, Section IV, Chapter 2 4; Sobota et al., 2024 6; API 2025 catalog 8.

Common questions

Is the acid dew point the same as the water dew point?
No. DOE gives the water dew point of natural gas combustion products as about 135 °F (57 °C), while its minimum flue gas temperatures, set to prevent condensation and stack corrosion, start at 250 °F (121 °C).
Does burning natural gas avoid dew point corrosion?
Not entirely. DOE still sets a 250 °F (121 °C) minimum for natural gas, and condensate from natural gas combustion is acidic.
Is dew point corrosion the same as cold-end corrosion?
They describe the same problem: corrosion at the coldest end of the flue gas path. DOE and the 2023 boiler study both use the term cold-end corrosion.

Beacon explains these concepts in its own words for education. It does not reproduce or replace the standards cited, and Winda is not affiliated with or endorsed by the organizations that publish them. Engineering decisions need the current edition of the standard and a qualified engineer.

Sources

  1. 1.Energy Tips: Steam, Steam Tip Sheet #3: Use Feedwater Economizers for Waste Heat Recovery (DOE/GO-102012-3412) · US Department of Energy, Advanced Manufacturing Office
  2. 2.Energy Tips: Steam, Steam Tip Sheet #26B: Considerations When Selecting a Condensing Economizer (DOE/GO-102012-3397) · US Department of Energy, Advanced Manufacturing Office
  3. 3.AP-42, Compilation of Air Emissions Factors, Section 1.3: Fuel Oil Combustion · US Environmental Protection Agency (EPA)
  4. 4.OSHA Technical Manual, Section IV, Chapter 2: Petroleum Refining Processes · US Occupational Safety and Health Administration (OSHA)
  5. 5.Cold-end corrosion caused by hygroscopic ammonium chloride in thermal conversion of biomass and waste (E. Vainio, P. Yrjas, L. Hupa, M. Hupa), Fuel 346, 128061 · Åbo Akademi University (research portal record, CC BY) ·
  6. 6.CFD modelling of the air preheater fired with gas mixture to find the cause of the preheater damage (T. Sobota, D. Taler, M. Granda, M. Szymkiewicz), E3S Web of Conferences 551, 01001 · EDP Sciences (CC BY 4.0)
  7. 7.Improving Process Heating System Performance: A Sourcebook for Industry, Third Edition · US Department of Energy, Advanced Manufacturing Office
  8. 8.2025 Publications Catalog (entry for RP 573) (RP 573, 4th edition, January 2021) · American Petroleum Institute (API)
  9. 9.Energy Tips: Steam, Steam Tip Sheet #26A: Consider Installing a Condensing Economizer (DOE/GO-102012-3393) · US Department of Energy, Advanced Manufacturing Office